Material Notes:
MarkeTech International special honeycomb ceramics have a uniform lattice structure, low expansion coefficient, good thermal shock resistance, higher specific surface area, low-pressure drop, and low density. They are available in cordierite or mullite ceramic. Cordierite honeycomb ceramics are mainly used as catalyst support for the automobile and for purification waste gas of industrial organic processing, and as filters in melting metal.
Physical Properties Metric English Comments
Density 0.500 g/cc
0.0181 lb/in³
Water Absorption 25 - 30 %
25 - 30 %
Porosity 45 - 50 %
45 - 50 %
Specific Surface Area 5.0 - 10 m²/g
5.0 - 10 m²/g
Mechanical Properties Metric English Comments
Compressive Strength >= 4.00 MPa
>= 580 psi
Perpendicular to holes
>= 12.0 MPa
>= 1740 psi
Parallel to holes
Thermal Properties Metric English Comments
CTE, linear 1.50 - 1.80 µm/m-°C
0.833 - 1.00 µin/in-°F
Melting Point 1360 °C
2480 °F
Descriptive Properties Value Comments
Hole Density 200/inch
Wall Thickness 0.3 mm
Users viewing this material also viewed the following: