Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
NYCOA 5033 HST 33% Glass-Fiber Reinforced, Heat Stabilized, Translucent Nylon 66 Resin NYCOA 5033 HST is a 33% glass fiber reinforced, heat stabilized, translucent Nylon 66 resin used for injection molding. It has been specifically formulated for see through storage tanks for automoti.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
PolyOne Nymax™ GF 1200 33 Red 31 A Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
Ravago Manufacturing Americas Hylon® N2233HL BK Nylon 6 Available in North America Filler: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantForm: Pellets Proces.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible FC801 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
PolyOne Edgetek® AT-000/000 HI5 Natural NA Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | Method A; ASTM D792 |
LNP Thermocomp® EC-1006 Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
RTP Company RTP 207D Z Nylon 6/12 (PA 6/12) Glass Fiber 40% - FDA Type
(discontinued **)&l Glass Fiber 40% - FDA TypeComments:Glass FiberFDA CompliantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided .. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
LG Chemical LUCEL HI510 POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: Gears, Automobile ClipCAS No. 66455-31-0Information provided by LG Chemical |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
LG Chemical LUCEL HI520 POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ISO 1183 |
GEHR Plastics POM-ELS Acetal, Electrically Conductive Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear be.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | |
Sylvin Technologies 9077-80 LMW Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RB006 PA 66 LNP* THERMOCOMP* RB006 is a compound based on Nylon 66 resin containing 30% Glass Bead. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
Teknor Apex APEX® 80128-Y Polyvinyl Chloride, Flexible Notes: 75°C Insulation; RoHS CompliantFeatures: Sunlight Resistant (720 hours) Uses: Cable Jacketing; InsulationAgency Ratings: UL QMTT2 .E73402; UL 1063; UL 1581; UL 62; UL 83Forms: Pellets Wire.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
Chase Plastics CP Pryme® N130GL (COND, 50% RH) Nylon 6, 30% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ ASC-331 Inorganic Antislip Masterbatch Based in Polyethylene DescriptionPOLYBATCH® ASC-331 is an inorganic antislip masterbatch based in polyethylene. ApplicationThis masterbatch was designed for use in moderate to heavy gauge applications to increase film .. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Brown 1028 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 1028 is a brown color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® .. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ ASC-331 Inorganic Antislip Masterbatch Based in Polyethylene DescriptionPOLYBATCH® ASC-331 is an inorganic antislip masterbatch based in polyethylene. ApplicationThis masterbatch was designed for use in moderate to heavy gauge applications to increase film .. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D 792 |
RTP Company PermaStat® 302 FR Polycarbonate (PC), ESD Protection - Permanently Anti-static - Glass Fiber - Flame Retardant |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Cedar 10310U Concentrate Based In LLDPE DescriptionPOLYBATCH® Cedar 10310U is a cedar color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stabi.. |
|||
Specific Gravity | 1.38 - 1.44 g/cc | 1.38 - 1.44 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-14961 30% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall 14890 Wire & Cable Flexible PVC General purpose UL approved 720 hour sunlight resistant jacket suitable for a maximum 80°C temperature rating at a 1/32" wall. Recommended for UF-B and NM-B constructions and also RG59 coaxial cab.. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall 17870 Wire & Cable Flexible PVC TW, THW insulation compound. Oil II rated. 720 hour sunlight resistant in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D-792 |
Axiall 3014 Rigid PVC, Extrusion Georgia Gulf 3014 is a base for use of wood flour up to 40 percent. Impact Strength & ToughnessFlame RetardantChemical ResistanceDimensional StabilityInformation provided by Georgia GulfGeorgia Gul.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | silicone property; Arlon SQA-TMS-024 |
Arlon 55096R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 2523 fiberglass; Side 2: uncured silicone rubber |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
Colorite Polymers 4875 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | |
Trelleborg Commercial Neoprene® C433 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Norwegian Wood 60242U/3 Concentrate Based In LLDPE DescriptionPOLYBATCH® 60242U/3 is a norwegian wood color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D 792 |
RTP Company RTP 903 Z Polysulfone (PSU), Glass Fiber - FDA Compliant Ingredients |