Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 72.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C

@Temperature -18.0 - 38.0 °C
40.0 µin/in-°F

@Temperature -0.400 - 100 °F
ASTM D696
Plaskolite Duraplex® SG-05 Sign Grade Acrylic Sheet, Impact Modified
Available in unlimited lengths - no seams in finished products.Data provided by the manufacturer, Plaskolite, Inc.
CTE, linear 72.0 µm/m-°C
40.0 µin/in-°F
ASTM D696
Quantum PBT
Information provided by Quantum Advanced Engineering Plastics
CTE, linear 72.0 - 144 µm/m-°C
40.0 - 80.0 µin/in-°F
Average value: 94.5 µm/m-°C Grade Count:17
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
CTE, linear 72.0 - 90.0 µm/m-°C

@Temperature 0.000 - 156 °C
40.0 - 50.0 µin/in-°F

@Temperature 32.0 - 312 °F
Average value: 76.5 µm/m-°C Grade Count:4
Overview of materials for Acrylic, Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o..
CTE, linear 72.0 µm/m-°C

@Temperature -18.0 - 38.0 °C
40.0 µin/in-°F

@Temperature -0.400 - 100 °F
ASTM D696
Plaskolite Optix® PL-76 Acrylic Resin  (discontinued **)
Injection/extrusion pellets. Medium heat resistance with higher flow than PL-52 pellets.Data provided by the manufacturer, Plaskolite, Inc.
CTE, linear 72.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
40.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM-D696
Ineos ABS Lustran® Guardian™ 732 ABS, Extrusion Grade
Lustran® Guardian™ ABS 732 is an extrusion grade resin designed for use in thermoformed refrigerator and freezer liner applications. It is suitable for use with 245fa PU foams.
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech 513 Static Dissipative Control Sheet
Description: Static Control SheetInformation provided by Spartech.
CTE, linear 72.0 µm/m-°C
40.0 µin/in-°F
ASTM D 696
Styrolution PS 1290/1291 GPPS
Extrusion / thermoforming foam sheetLow residual styrene monomer contentHigh melt strength and stiffnessUL Classification 94 HB for 1290Information provided by Styrolution
CTE, linear 72.0 µm/m-°C
40.0 µin/in-°F
ASTM D 696
Styrolution PS 1600 GPPS
Foam extrusion; Injection moldingGood balanced of strength, flow and heat resistanceFree of zinc and oil additivesInformation provided by Styrolution
CTE, linear 72.0 µm/m-°C

@Temperature -40.0 - 82.2 °C
40.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron Pulse® 2200BG ABS + PC
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
CTE, linear 72.0 µm/m-°C
40.0 µin/in-°F
ASTM D 696
Styrolution PS 2610 GPPS
Extruded packaging; Thermoforming applicationsExcellent toughnessHigh melt strengthGood flow and processabilityInformation provided by Styrolution
CTE, linear 72.0 - 180 µm/m-°C
40.0 - 100 µin/in-°F
TriStar Ultracomp UC-400 Composite Bearing
Ultracomp UC-400 - Designed for high loads, low speeds, impact and vibration applications. UC-400 has a MOS2 additive for salt water applications where cathodic reactions could occur. Excellent dry ..
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 100 °C
40.0 µin/in-°F

@Temperature 32.0 - 212 °F
Evonik CYRO Acrylite Plus® H-16 Acrylic Molding Compound
This material has been replaced by Acrylite Plus® ZK-6 - same physical properties with lower haze. Data provided by CYRO IndustriesUses: auto lenses and trim, glazing, sanitary ware, engraving sto..
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 100 °C
40.0 µin/in-°F

@Temperature 32.0 - 212 °F
Evonik CYRO Acrylite Plus® H-17 H Acrylic Molding Compound
Data provided by CYRO IndustriesUses: medical devices
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 100 °C
40.0 µin/in-°F

@Temperature 32.0 - 212 °F
ASTM D696
Evonik CYRO Acrylite Plus® zk4BR Impact Acrylic Polymer
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 156 °C
40.0 µin/in-°F

@Temperature 32.0 - 312 °F
ASTM D696
Evonik CYRO ACRYLITE PLUS® ZK-6 Impact Acrylic Polymer
ACRYLITE PLUS® ZK-6 impact acrylic polymer is an amorphous, impact-modified thermoplastic molding and extrusion compound based on polymethyl methacrylate (PMMA).Typical properties of ACRYLITE PLUS®..
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 100 °C
40.0 µin/in-°F

@Temperature 32.0 - 212 °F
ASTM D696
Evonik CYRO Acrylite Plus® zk6HF Impact Acrylic Polymer
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 100 °C
40.0 µin/in-°F

@Temperature 32.0 - 212 °F
ASTM D696
Evonik CYRO Acrylite® 8N df 21 Acrylic Polymer
Superior light diffusion and transmittance is obtained by incorporation of spherical, high MW polymer beads of a different refractive index into the acrylic matrix. Used in lighting, optoelectronics..
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 100 °C
40.0 µin/in-°F

@Temperature 32.0 - 212 °F
ASTM D696
Evonik CYRO Acrylite® 8N df 23 Acrylic Polymer
Superior light diffusion and transmittance is obtained by incorporation of spherical, high MW polymer beads of a different refractive index into the acrylic matrix. Used in lighting, optoelectronics..
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 100 °C
40.0 µin/in-°F

@Temperature 32.0 - 212 °F
ASTM D696
Evonik CYRO ACRYLITE® H15 Acrylic Polymer
ACRYLITE® H15 acrylic polymer is an amorphous thermoplastic molding and extrusion compound based on polymethyl methacrylate (PMMA).Typical properties of ACRYLITE® acrylic polymers are excellent we..
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Evonik CYRO Acrylite® SG Acrylic Sheet, Sign Grade
Data provided by CYRO IndustriesContinuously manufactured sheet developed for the sign market. Versatile, tough, lightweight, easy to fabricate and machine. Cutting, routing, drilling, forming, an..
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Ensinger Tecast Vekton™ 6PA Black Unfilled Cast Nylon 6 (PA6)
Tecast® 6PA Black is a black cast nylon that is more UV resistant than natural nylon 6.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combina..
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Ensinger Tecast Vekton™ 6PAL Oil-Filled Cast Nylon 6 (PA6)
Tecast® 6PAL is used in applications requiring excellent bearing and wear properties where external lubrication is difficult or impractical.General Tecast® Cast Nylon Information: Tecast cast nylo..
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Axiall 8240 Rigid PVC, Extrusion
Georgia Gulf 8240 is a general-purpose rigid PVC extrusion compound designed for applications requiring the following properties: Rigidity/StiffnessGlossImpact Strength & ToughnessFlame RetardantCh..
CTE, linear 72.0 - 162 µm/m-°C

@Temperature 25.6 - 204 °C
40.0 - 90.0 µin/in-°F

@Temperature 78.0 - 400 °F
ASTM D696
Technetics Group Texolon™ 8764 PTFE  (Unverified Data**)
A premium PTFE sheet manufactured from the highest quality PTFE.PTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Dielectri..
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 50.0 °C
40.0 µin/in-°F

@Temperature 32.0 - 122 °F
DIN 53752A
Evonik CYRO Rohaglas® 99524 Clear Acrylic Film
ROHAGLAS® Film 99524 acrylic film, based upon polymethyl methacrylate and acrylic elastomers, offers crystal-clear optical properties with two glossy (Class A) surfaces. Its excellent abrasion resi..
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Axiall 3240 Rigid PVC, Extrusion
Georgia Gulf 3240 is a special purpose rigid powder blend PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChe..
CTE, linear 72.0 - 72.0 µm/m-°C

@Temperature 0.000 - 156 °C
40.0 - 40.0 µin/in-°F

@Temperature 32.0 - 312 °F
Average value: 72.0 µm/m-°C Grade Count:2
Overview of materials for Acrylic, UV Stabilized, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, UV Stabilized, Molded". Each property range of values reported is minimum and maximum values of..
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech Spectar® UV Copolyester Sheet
Description: Copolyester SheetSpectar is a registered trademark of Eastman Chemical Company.Information provided by Spartech.
CTE, linear 72.0 - 100 µm/m-°C
40.0 - 55.6 µin/in-°F
Average value: 88.4 µm/m-°C Grade Count:7
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim..
Copyright © lookpolymers.com All Rights Reserved