Material Notes:
AA-BOND 201 is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. AA-BOND 201 is versatile two-part epoxy system contains no solvents, mixes easily at room temperature, and is suitable for high performance structural bonding applications where the combination of very fast room temperature curing coupled with low shrinkage and excellent mechanical and electrical properties is needed. AA-BOND 201 develops strong, tough bonds to metals, plastics, glass and glass fabrics, hardboards and forestry products, ceramics, rubber, masonry materials, and other construction materials. AA-BOND 201 is an excellent electrical insulator, and provides superior resistance to vapors and gases, water, galvanic action, petroleum fuels, salt solutions, and many other organic and inorganic compounds. AA-BOND 201 develops significant properties 1 hour after mixing. However, an extended cure of 4-6 hours at 25°C is required for fully matured bonds.Appearance: Hazy, light strawCure Type: Heat cure or Room TemperatureBenefits:Resistant to many organic/inorganicsStrong bond strengthGreat electrical insulatorDurable Mix Ratio by weight: 100:93/Resin:HardenerSubstrates: Metals, ceramics, glass, glass fabrics, wood leather, rigid plastics, marble, stone, rock, concrete, sheetrock, plaster, cement and tile.Typical Application: Anything requiring the unique properties this adhesive offersInformation provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
mixed, uncured
Solids Content 100 %
100 %
uncured
Viscosity 3600 cP
3600 cP
Uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 25
25
Adhesive Bond Strength 1.38 MPa
200 psi
Izod Impact, Notched 1.01 J/cm
1.90 ft-lb/in
Thermal Properties Metric English Comments
CTE, linear 59.9 µm/m-°C
33.3 µin/in-°F
Maximum Service Temperature, Air 115 °C
239 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 25.0 °C
77.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+11 ohm-cm
5.00e+11 ohm-cm
Dielectric Constant 4.8
4.8
Dielectric Strength 16.1 kV/mm
410 kV/in
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 65.0 °C
0.500 hour

@Temperature 149 °F
30.0 min

@Temperature 65.0 °C
0.500 hour

@Temperature 149 °F
120 min

@Temperature 25.0 °C
2.00 hour

@Temperature 77.0 °F
Pot Life 3.00 min
3.00 min
uncured
Shelf Life 12.0 Month
12.0 Month
uncured