Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Pot Life = 3.00 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 3.00 min
3.00 min
Northstar Polymers MSB-A95A High Performance Polyurethane Cast Elastomer System
This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio..
Pot Life 3.00 min
3.00 min
Northstar Polymers MSS-A70GQ High Performance Polyurethane Cast Elastomer System 70A
This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires cut/tear resistance, dry-abrasion resistance, slow resp..
Pot Life 3.00 - 4.00 min

@Temperature 20.0 °C
3.00 - 4.00 min

@Temperature 68.0 °F
Permabond ET500 Epoxy Resin
PERMABOND ET500 is a two-part fast-setting epoxy adhesive which bonds to a wide variety of substrates such as wood, metal, ceramics and some plastics and composites. It cures rapidly at room tempera..
Pot Life 3.00 min

@Temperature 23.9 °C
3.00 min

@Temperature 75.0 °F
3M Scotch-Weld™ 3535 B/A Off-white Two-Part Urethane Adhesive 3535 B/A Off-white  (discontinued **)
Two-part urethane adhesives cure at room temperature or with heat to provide tough, impact resistant bonds with high peel strength. Features include fast cure adhesive, 15-20 minutes handling stren..
Pot Life 3.00 min
3.00 min
Northstar Polymers MPG-D70A Room-Temperature-Curable Polyurethane Casting Elastomer
MPG-D70A is room-temperature-curable polyurethane casting elastomer system designed for molding polyurethane parts with tough, but flexible physical characteristics. The typical applications for th..
Pot Life 3.00 min

@Temperature 23.9 °C
3.00 min

@Temperature 75.0 °F
ITW Devcon Rubber Repair / Castable Urethane High Temp Edge & Seal (T-36), Amber
Information provided by ITW Devcon
Pot Life 3.00 min

@Temperature 23.9 °C
3.00 min

@Temperature 75.0 °F
ITW Devcon Rubber Repair / Castable Urethane Edge & Seal (T-35), Black
Information provided by ITW Devcon
Pot Life 3.00 min
3.00 min
uncured
Atom Adhesives AA-BOND 201 Epoxy Adhesive
AA-BOND 201 is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. AA-BOND 201 is versatile two-part epoxy system..
Copyright © lookpolymers.com All Rights Reserved