Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers NPS 90-0802 Polystyrene Description: Injection Molding Grade, High ImpactInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm |
1.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Oxford Polymers PBT 30GF PBT, 30% Glass Fiber Reinforced Product Description: Glass Fiber (30% Reinforced), PBT injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents and LubricantsSpecial Characteris.. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | ASTM D256 |
Ravago Manufacturing Americas Hylon® N1025HLFR Nylon 6/6, 25% Fiberglass, Heat Stabilized, Lubricated, Flame retardant (Cond) Information provided by Ravago. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | 1/8" (3mm) notched bar; ASTM D256 |
Ineos N12N-00 Polypropylene Impact Copolymer Grade N12N-00 is a nucleated polypropylene impact copolymer with an excellent balance of stiffness and impact resistance for injection molding applications and compounding products used in Lawn and .. |
|||
Izod Impact, Notched | 1.01 J/cm @Diameter 3.17 mm |
1.90 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos R12C-01 Polypropylene Random Copolymer Grade R12C-01 is a high clarity, antistatic polypropylene copolymer for injection molding and stretch blow molding applications. This material meets the requirements of the U.S. Food and Drug Admini.. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | |
MTI ThermoStran® PP-30C Long Carbon Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | ASTM D 256 |
Shakespeare Isocorâ„¢ CU145SI Nylon 6/66 Isocorâ„¢ CU145SI is a high viscosity, plasticized, PA-6/66 copolymer resin. This resin is specifically suited for applications requiring excellent abrasion resistance while maintaining a balan.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm |
1.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 E GF33 LE 33% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightFeatures: Low ExtractablesProcessing Method: ExtrusionInformation provided by TP Composi.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm |
1.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF33 HR L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: Lubricated and Hydrolysis Resistant TPCI# 9357101Informatio.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm |
1.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS IM TM20 20% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingInformation p.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm |
1.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® HIPS TL10 BK Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant (10%)Features: Good Wear Resistance, Low Friction and LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm |
1.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN® EG106 ABS Inherently Static Dissipative and Glass Fiber reinforced ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by Plastx.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ASA S210 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ModulusInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ASA T-115 Description: ASA Weatherable Polymer, Injection Molding Grade, High Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0436W20L Wollastonite Reinforced |
|||
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylene® P6-30FG-1804 30% Glass Fiber Reinforced, Heat and UV Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylene® P7-30FG-0874 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | ASTM D256 Type A |
Quadrant EPP Proteus® White Homopolymer Polypropylene (ASTM Product Data Sheet) |
|||
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylon® LSG-440A 60% Ceramic and Glass Fiber Reinforced Information provided by Asahi Thermofil |