Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 59.9 - 75.0 µm/m-°C | 33.3 - 41.7 µin/in-°F | Average value: 65.0 µm/m-°C Grade Count:3 |
Overview of materials for Acrylic, Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o.. |
|||
CTE, linear | 59.9 µm/m-°C @Temperature 20.0 °C |
33.3 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Diapolyacrylate Acrypet® MF-001 PMMA Acrypet® is a registered trade mark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers. |
|||
CTE, linear | 59.9 µm/m-°C @Temperature 20.0 °C |
33.3 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Diapolyacrylate Acrypet® VH-001 Heat Stabilized PMMA Acrypet® is a registered trade mark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers. |
|||
CTE, linear | 59.9 µm/m-°C | 33.3 µin/in-°F | |
Atom Adhesives AA-BOND 201 Epoxy Adhesive AA-BOND 201 is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. AA-BOND 201 is versatile two-part epoxy system.. |
|||
CTE, linear | 59.9 µm/m-°C | 33.3 µin/in-°F | |
Atom Adhesives AA-BOND F110 Epoxy Adhesive AA-BOND F110 is a rigid, optically clear adhesive with a very low viscosity. AA-BOND F110 is room temperature system an excellent choice for thin bond-line assembly and repair applications of prisms.. |
|||
CTE, linear | 59.9 µm/m-°C | 33.3 µin/in-°F | |
Atom Adhesives AA-BOND F125 Epoxy Adhesive AA-BOND F125 is a 8 minutes gelling epoxy recommended for use in fiber optic connectors, optical and industrial bonding applications. AA-BOND F125 is clear, two part system is easily mixed and used .. |