Material Notes:
A 25% glass reinforced high impact Nylon 6 designed for applications requiring a high level of toughness, as well as superior low temperature properties.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 125 MPa
18100 psi
ATSM D638
Flexural Modulus 5.30 GPa
769 ksi
ASTM D790
Izod Impact, Notched 1.66 J/cm
3.11 ft-lb/in
ASTM D256
1.13 J/cm

@Temperature -40.0 °C
2.12 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D648