Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.66 J/cm | 3.10 ft-lb/in | @ 73°F; ASTM D256 |
Rochling Engineered Plastics Polystone® G HDPE Extruded Sheet Information provided by Röchling Engineered Plastics. |
|||
Izod Impact, Notched | 1.66 J/cm @Temperature -30.0 °C |
3.11 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Izod Impact, Notched | 1.66 J/cm @Temperature -30.0 °C |
3.11 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Asia Pacific) 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Izod Impact, Notched | 1.66 J/cm @Temperature -30.0 °C |
3.11 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Europe-Africa-Middle East) 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Izod Impact, Notched | 1.66 - 1.87 J/cm | 3.10 - 3.50 ft-lb/in | Average value: 1.77 J/cm Grade Count:3 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |
|||
Izod Impact, Notched | 1.66 J/cm @Temperature -30.0 °C |
3.10 ft-lb/in @Temperature -22.0 °F |
PB; ASTM D256 |
LyondellBasell SEQUEL® E3000 TPO Description: SEQUEL® E3000 thermoplastic olefinic elastomer (TPO) is designed for thermoformed exterior and interior applications that require toughness and dimensional stability. This extrusion.. |
|||
Izod Impact, Notched | 1.66 J/cm @Thickness 3.17 mm |
3.11 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LG Chemical Lupox® PBT-HI1002FM Impact Modified, Flame Retardant PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 1.66 J/cm | 3.11 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX9406P PPE+HIPS (Asia Pacific) Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 125dc HDT. UL94 V-0 rated. Electrical applications. |
|||
Izod Impact, Notched | 1.66 J/cm @Thickness 3.17 mm |
3.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® HDPE GF30 CC 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.66 J/cm @Thickness 3.17 mm |
3.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF33 HS L BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat Stabilizer Features: Lubricated and Heat StabilizedProcessi.. |
|||
Izod Impact, Notched | 1.66 J/cm @Thickness 3.17 mm |
3.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF40 A1 BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant Features: Lubricated, Low Shrinkage and Good Wear ResistanceAppearan.. |
|||
Izod Impact, Notched | 1.66 J/cm @Thickness 3.17 mm |
3.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF50 HS L BK 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Izod Impact, Notched | 1.66 J/cm | 3.11 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DX10313 PC (Asia Pacific) DX10313 is high modulus polycarbonate, 50% glass filled, with balanced flow and impact strength |
|||
Izod Impact, Notched | 1.66 J/cm @Thickness 3.17 mm |
3.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0320 High Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 1.66 J/cm @Thickness 3.17 mm |
3.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0320 High Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 1.66 J/cm | 3.11 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF008 PA 66 LNP* THERMOCOMP* RF-1008 is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
Izod Impact, Notched | 1.66 J/cm @Temperature -40.0 °C |
3.11 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing 20% Long Glass Fiber. Added features of this material include: Easy Molding, Structural. |
|||
Izod Impact, Notched | 1.66 J/cm @Temperature -40.0 °C |
3.11 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Europe-Africa-Middle East) LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched | 1.66 J/cm | 3.11 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON FX91304 PE LNP* STAT-KON* FX91304 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Izod Impact, Notched | 1.66 J/cm | 3.11 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF008XXH PA 66 LNP* THERMOCOMP* RF008XXH is a compound based on Nylon 66 resin containing 40% Glass Fiber. Added feature of this material includes: Healthcare. |
|||
Izod Impact, Notched | 1.66 J/cm @Thickness 3.17 mm |
3.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN®-V 660SF ABS High Flow ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 1.66 J/cm | 3.10 ft-lb/in | 0.125 in; ASTM D256 |
Chase Plastics CP Pryme® NNN260L (Dry) Nylon 66/6 Copolymer, 60% Glass Fiber Reinforced Features: Good chemical resistanceGood compressive strengthGood creep resistanceGood dimensional stabilityGood flowGrease resistantOil resistantHigh rigiditySolvent resistantHigh tensile strengthHig.. |
|||
Izod Impact, Notched | 1.66 J/cm | 3.10 ft-lb/in | ASTM D256 |
ExxonMobil PP7684KN Impact Copolymer Product Description: A high crystallinity, high impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for injection molded small and large appliance .. |
|||
Izod Impact, Notched | 1.66 J/cm | 3.10 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0437G25M5CL Glass/Mineral Reinforced Coupled |
|||
Izod Impact, Notched | 1.66 J/cm | 3.10 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0437W40L1 Wollastonite Reinforced |
|||
Izod Impact, Notched | 1.66 J/cm | 3.10 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0436G30CL Glass Reinforced |
|||
Izod Impact, Notched | 1.66 J/cm | 3.11 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 827L-25G Nylon 6, 25% Glass Reinforced A 25% glass reinforced high impact Nylon 6 designed for applications requiring a high level of toughness, as well as superior low temperature properties.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.66 J/cm @Temperature -40.0 °C |
3.11 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Asia Pacific) LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched | 1.66 J/cm | 3.10 ft-lb/in | ASTM D256 |
PlastxWorld CEVIAN® A2603 15% GF PA/ABS Alloy, Conditioned Property data is for samples equilibrium moisture (1.1%)These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld.. |