Polymer Property : Tensile Strength, Ultimate = 18100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 125 MPa
18100 psi
Same value from ASTM and ISO tests; 5 mm/min.
BASF Capron® GR15 HS 15% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron GR15 HS is a heat stabilized 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest..
Tensile Strength, Ultimate 125 - 230 MPa
18100 - 33400 psi
Average value: 182 MPa Grade Count:27
Overview of materials for Nylon 66, 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in..
Tensile Strength, Ultimate 125 MPa
18100 psi
Hybrid Plastics Nanoreinforced® PM 1215 Polyimide
The homogeneous dispersion of POSS® cages within polyimide provides enhanced control over chain dynamics which increases the toughness and damage tolerance over conventional polyimide. The chemic..
Tensile Strength, Ultimate 125 MPa
18100 psi
ISO 527
Wellman Wellamid® GF14-60 XE-N 14% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
Tensile Strength, Ultimate 125 MPa
18100 psi
ISO 527
Wellman Wellamid® MRGF25/15 22H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 66, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Tensile Strength, Ultimate 125 MPa
18100 psi
Wieland 1964 Wilaform Gold
Fine gold. Universally applicable for sheet metals, volumes, pipes, profiles and contacts.Applications: chains, coin/shape, pipesDental
Tensile Strength, Ultimate 125 MPa
18100 psi
cond; ISO 527-1/-2
DSM Akulon® S223-PG8 PA66-GF40
40% Glass Reinforced, Impact Modified
Tensile Strength, Ultimate 125 MPa

@Temperature 120 °C
18100 psi

@Temperature 248 °F
ISO 527-1/-2
DSM Stanyl® 46HF4530 PA46-GF30
30% Glass Reinforced, Heat Stabilized, High Flow, for E&E applications
Tensile Strength, Ultimate 125 MPa
18100 psi
cond; ISO 527-1/-2
DSM Stanyl® OCD2100 BK27021 PA46-GF40
40% Glass Reinforced, Heat Stabilized
Tensile Strength, Ultimate 125 MPa

@Temperature 120 °C
18100 psi

@Temperature 248 °F
ISO 527-1/-2
DSM Stanyl® TW200B6 PA46-CF30
30% Carbon Reinforced, Heat Stabilized, Lubricated
Tensile Strength, Ultimate 125 MPa
18100 psi
dry; ISO 527-1/-2
DSM Akulon® K224-G3-FC NA99001 PA6-GF15
15% Glass Reinforced
Tensile Strength, Ultimate 125 MPa
18100 psi
5mm/min; ISO 527
BASF Petra® 130 FR BK-112 30% Glass Filled PET
Petra 130 FR BK-112 is a 30% glass fiber reinforced, black pigmented, flame retardant injection molding compound based on post-consumer and post-industrial recycle polyethylene erephthalate feedstoc..
Tensile Strength, Ultimate 125 MPa
18100 psi
5mm/min; ISO 527
BASF Ultramid® 1403-2 BK ND3007 PA66 (Dry)
Tensile Strength, Ultimate 125 MPa
18100 psi
5mm/min; ISO 527
BASF Ultramid® 1403-2 NF3001 13% Glass Filled PA66 (Dry)
Ultramid 1403-2 NF3001 is a 13% glass reinforced, heat stabilized injection molding PA6/6.
Tensile Strength, Ultimate 125 MPa
18100 psi
5mm/min; ISO 527
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Conditioned)
Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also..
Tensile Strength, Ultimate 125 MPa
18100 psi
5mm/min; ISO 527
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry)
Ultramid 8267G HS BK-102 is a heat stabilized, black pigmented, 40% mineral and glass fiber reinforced nylon 6 injection molding compound. It possesses a balance of engineering properties in combin..
Tensile Strength, Ultimate 125 MPa
18100 psi
ASTM D638
A. Schulman ComAlloy Hiloy® 622 Nylon 6/6, Glass Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Tensile Strength, Ultimate 125 MPa
18100 psi
ASTM D638
A. Schulman ComAlloy Voloy® 413 Polyester - PBT, Glass Reinforced, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Tensile Strength, Ultimate 125 MPa
18100 psi
ASTM D638
A. Schulman ComAlloy Voloy® 430 Glass Reinforced, PBT Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Tensile Strength, Ultimate 125 MPa
18100 psi
5mm/min; ISO 527
BASF Ultradur S 4090 G6 LS High Speed BK15077 30% Glass Filled PBT
Ultradur S 4090 G6 LS High Speed BK15077 is a high flow, fast cycling with low warpage, 30% glass filled injection molding PBT.
Tensile Strength, Ultimate 125 MPa
18100 psi
ATSM D638
Ashley Polymers Ashlene® 827L-25G Nylon 6, 25% Glass Reinforced
A 25% glass reinforced high impact Nylon 6 designed for applications requiring a high level of toughness, as well as superior low temperature properties.Data provided by the manufacturer
Tensile Strength, Ultimate 125 MPa
18100 psi
ASTM D638
A. Schulman ComAlloy Hiloy® 626 Nylon 6/6, Glass/Mineral Reinforced
Data provided by the manufacturer, ComAlloy International Company.35% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Tensile Strength, Ultimate 125 MPa
18100 psi
ASTM data at 5 mm/min.
BASF Capron® 8233G 33% Glass-Filled Nylon 6 (Conditioned)  (discontinued **)
Capron 8233G is a 33% glass fiber reinforced polyamide 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also available in he..
Tensile Strength, Ultimate 125 MPa
18100 psi
Same value from ASTM and ISO tests; 5 mm/min.
BASF Capron® GR15 15% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron GR15 is a 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also..
Tensile Strength, Ultimate 125 MPa
18100 psi
ISO 527
LATI LAESTRA G/40 40% Glass Fiber Reinforced Syndiotactic Polystyrene (SPS)  (discontinued **)
Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270..