Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Conditioned (2.5% Moisture)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Conditioned (2.5% Moisture).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. Glass-reinforced Vydyne resins provide a higher heat distortion temperature, better resistance to creep, higher impact and better dimensional stability when compared with unreinforced PA66. These products have good chemical resistance to a broad range of chemicals, including many aliphatic and aromatic hydrocarbons found in most solvent, gasoline, hydraulic fluids, greases and machine oils. Vydyne R543H resin has tensile strength and modulus properties just below aluminum and zinc and can replace these metals in numerous applications due to an excellent balance of properties. Reduction in production costs, energy consumption and part weigh tare key advantages of Vydyne glass-reinforced PA66 resins over aluminum and/or zinc die-cast parts. Vydyne R543H is formulated to minimize the oxidative and thermal degradation of the PA66 polymer when exposed to elevated temperatures for extended periods of time. Vydyne R543H provides improved retention of physical properties under exposure to long-term heat. The continuous operating use temperature is 275°F, with short-term peak temperature as high as 475°F.Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Heat StabilizerLubricant Features:Gasoline ResistanceGood Chemical ResistanceGood Creep ResistanceGood Dimensional StabilityGood FlowGood Impact ResistanceGood Mold Release Grease ResistantHeat StabilizedHigh RigidityHigh StrengthHigh Tensile StrengthLubricated Oil ResistantSolvent ResistantUses: Automotive Under the Hood GearsHousings Lawn and Garden EquipmentPower/Other ToolsAppearance: Natural ColorForms: PelletsProcessing Method: Injection Molding
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ISO 1183
Water Absorption 0.60 %

@Time 86400 sec
0.60 %

@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 1.5 %
1.5 %
50% RH; ISO 62
Linear Mold Shrinkage 0.0040 cm/cm

@Thickness 2.00 mm
0.0040 in/in

@Thickness 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm

@Thickness 2.00 mm
0.0090 in/in

@Thickness 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 170 MPa
24700 psi
ISO 527-2
Elongation at Break 4.0 %
4.0 %
ISO 527-2
Tensile Modulus 11.3 GPa
1640 ksi
ISO 527-2
Flexural Strength 250 MPa
36300 psi
ISO 178
Flexural Modulus 9.40 GPa
1360 ksi
ISO 178
Izod Impact, Notched (ISO) 13.0 kJ/m²

@Temperature -30.0 °C
6.19 ft-lb/in²

@Temperature -22.0 °F
ISO 180
19.0 kJ/m²

@Temperature 23.0 °C
9.04 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched 9.00 J/cm²

@Temperature -30.0 °C
42.8 ft-lb/in²

@Temperature -22.0 °F
ISO 179
9.50 J/cm²

@Temperature 23.0 °C
45.2 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 1.40 J/cm²

@Temperature -30.0 °C
6.66 ft-lb/in²

@Temperature -22.0 °F
ISO 179
2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 179