Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.3 GPa | 1640 ksi | |
Plastcom SLOVAMID 66 GF 35 HTS PA66, 355% glass fibre, combined stability FeaturesPA 66 for injection moulding, chemically reinforced with 35% glass fibre, heat stabilized and stabilized against hydrolysis. Used for cooling water systems in the automotive industry. Delive.. |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | 5 mm/min; ASTM D638 |
LNP NORYL® EXCP0111 PPS + Polyphenylene Ether, 42% Glass / Mineral Reinforcement
(discontinued **) For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele.. |
|||
Tensile Modulus | 11.3 GPa @Temperature 23.0 °C |
1640 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | ISO 527 |
Nilit FRIANYL A63 V0 G5 Nylon 6.6 for injection molding, 25% glass fiber reinforced Nylon 6.6 for injection molding, flame retardant, free of halogen and phosphorus.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 11.31 GPa | 1640 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP UF0067W PPA LNP* THERMOCOMP* UF0067W is a compound based on Polyphthalamide resin containing 30% glass fiber. Added features of this material include: Hot Water Moldable, Non-Brominated & Non-Chlorinated Flam.. |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Asia Pacific) Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON MV00ASXC PP (Europe-Africa-Middle East) LNP* VERTON* MV00ASXC is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized. |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL EXNL1285 PPE+PS (Europe-Africa-Middle East) Noryl* EXNL1285 Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | ASTM D638 |
Plenco 3597 Phenolic, Granular, Injection Molded PLENCO 03597 is a mineral filled phenolic molding compound offering excellent flammability ratings even at thin cross sections, along with excellent arc and comparative track resistance values. UL r.. |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | ASTM D638 |
Plenco 4504 Phenolic, Granular, Compression Molded Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding c.. |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | dry; ISO 527-1/-2 |
DSM Akulon® N24-G7 PA6-GF35 35% Glass Reinforced |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Rynite® FR530 BK507 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Improved Flow Zytel HTNFR52G30NHF BK337 is a 30% glass reinforced flame retardant lubricated high performance.. |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® PLS 95G40DH1T BK261 Nylon 6
(Unverified Data**) 40% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G40DH1T is a 40% GR impact modified PA made with SHIELD technology its superior heatInformation provided by DuPont Performance Polymers |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | ISO 527 |
Azoty Tarnow™ TARNOFORM 300 GF7 POM 35% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | ISO 527 |
BASF Ultramid® 66 H2 G/35-V0KB NAT 0046 35% Glass Filled PA66 (Dry) Description: Ultramid 66 H2 G/35-V0KB NAT0046 is a 35% glass reinforced, heat stabilized injection molding grade. It is a V-0 self-extinguishing grade, with phosphorous. It offers good flowability a.. |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | ISO 527-2 |
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, Conditioned Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass.. |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, Conditioned Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, Conditioned Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, .. |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, Conditioned Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, Conditioned Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Conditioned (2.5% Moisture) Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Rynite® FR530L BK507 Polyethylene Terephthalate (PET) Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 11.3 GPa | 1640 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL FE1740PW PPE+PS (Europe-Africa-Middle East) Noryl* FE1740PW Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |