Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Thickness 4.00 mm, Temperature 23.0 °C |
6.19 ft-lb/in² @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180/1A |
Polimeri Europa Sinkral® PD L 322 ABS Resin Sinkral PD L 322 by continuous mass, is a general purpose, high flow injection molding grade having good impact resistance coupled with an excellent gloss.Applications: Widely used in the small and.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CE3210 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Nilit Nilamid A3 H G10 50% Glass Reinforced PA66 Description: Nilamid A3 H G10 (50% Glass Reinforced) is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance,.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPH4504 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Nilit Nilamid B3 H G10 50% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G10 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key characte.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML3021A PC (Europe-Africa-Middle East) LEXAN ML3021A is a high viscosity, UV stabilised grade especially designed for injection blow moulding and profile extrusion.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -40.0 °C |
6.19 ft-lb/in² @Temperature -40.0 °F |
50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6
(Unverified Data**) Zytel® ST7301 NC010 is a Super Tough, heat stabilized, lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and humidity.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612
(Unverified Data**) Zytel® 77G33L BK031 is a 33% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
LG Chemical EF-378 ABS, Flame Retardant, Halogen Free Information Provided by LG Chem |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 180-1U |
Lanxess Durethan® AM 40 X H2.0 901510 Nylon 66, Glass Fiber/Mineral Reinforced PA 66, 40% glass fibers/mineral, injection molding, heat-aging stabilized, low tendency to warpInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 180-1A |
Lanxess Durethan® BKV 40 H2.0 901510 Nylon 6, Glass Fiber Reinforced PA 6, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem HATX100 PEI+PCE (Europe-Africa-Middle East) Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Sax Polymers SAXAMID 126F7 Nylon 6, 35% Glass Fiber SAXAMID 126F7 is a polyamide 6 injection-molding-grade reinforced with 35% glass fibers. Because of its high strength and stiffness this grade is often used for stressed parts. Additional properties.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Europe-Africa-Middle East) Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the E.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp RF00AES PA 66 (Europe-Africa-Middle East) LNP THERMOCOMP* RF00AES is a compound based on PA66 resin containing Glass Fiber, Mold Release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl EN130S PPE+HIPS (Europe-Africa-Middle East) Noryl EN130S is an extrusion grade with a Vicat B/120 temperature of 140 deg C, developed for profile extrusion and in compliance with Food contact regulations; color limited.This data was supplied .. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 77G33HS1L NC010 Nylon 612 Zytel® 77G33HS1L NC010 is a 33% glass fiber reinforced, heat stabilized polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide BG6ST01 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG6ST01 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 179/1eA |
Eurostar Staramide RF00AES PA66/6, 50% Glass Filled, Injection Molded Staramide RF00AES is a 50% Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66 C 50V S3)Information provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, Conditioned Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R530H BK08 Nylon 66, 30% Glass Reinforced, Conditioned Vydyne® R530H BK08 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Conditioned Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, Conditioned Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® A3HG6 HR BK 23591 30% Glass Filled PA66 (Dry) Description: 30% glass-fiber reinforced injection-molding grade with enhanced hydrolysis resistance, e.g., for applications in vehicle cooling systems.Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R633H Nylon 66/6, 33% Glass Reinforced, DAM Vydyne® R633H is 33% glass-fiber reinforced PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold .. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXRL0681 PC Copolymer 25 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
BASF Nypel® 2351 HS BK PA6 (Dry) Description: Nypel® 2351 HS BK is a heat stabilized, pigmented black, impact modified PA6 extrusion grade compound. Quality and performance are combines at a lower cost. It is based on recycled PA6.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl EN130 PPE+HIPS (Europe-Africa-Middle East) NORYL EN130 is an extrusion material with a Vicat B/120 of 140 deg C according ISO 306. NORYL EN130 is a standard extrusion grade for applications where higher temperature resistance is required. NO.. |