Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® C8080REC PC+ABS (Europe-Africa-Middle East) PC+ABS, Industrial quality resin with good flow, good temperature resistance and moderate ImpactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Europe-Africa-Middle East) PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Europe-Africa-Middle East) Reinforced PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Asia Pacific) High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Europe-Africa-Middle East) High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
LG Chemical AF-348 ABS, Flame Retardant, Heat Resistant, Weather Resistant Information Provided by LG Chem |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-9522 20% Talc-Filled, Elastomer Modified Polypropylene Block-Copolymer INNOPOL® CS 2-9522 is a 20% talc-filled, elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-9522 is dev.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Mitsubishi Xantar® C CM 506 U Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eA |
Lanxess Durethan® AKV 30 HR H2.0 901510 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, hydrolysis stabilized, good heat-ageing resistance |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eA |
Lanxess Durethan® BC 304 H3.0 000000 Nylon 6 PA 6, injection molding grade, non-reinforced, elastomer-modified, extremely high notched impact strength, including in the dry state and at low temperatures, also applicable for barrier layers in e.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Lanxess Durethan® BKV 230 H2.0 901510 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 130, conditioning .. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Lanxess Durethan® DP 2325 H3.0 000000 Nylon 66 PA 66, injection molding grade, non-reinforced, elastomer-modified, good heat-ageing resistance, extremely high notched impact strength even at dry state and at low temperatures |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Mitsubishi Xantar® C CM 406 U Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis BC650MO Polypropylene Copolymer BC650MO is a very high impact polypropylene heterophasic copolymer intended for injection molding. This product offers a good UV resistance, further enhanced by pigmentation. This grade features hig.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -20.0 °C |
9.52 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis BL1481 High Density Polyethylene BL1481 is a semi high molecular weight polyethylene comprising an extra ordinary ESCR and very good chemical resistance This product is intended for blow molding. This grade is available in granular.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis RA130E-6034 Polypropylene Random Copolymer RA130E-6034 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis RA130E-2492 Polypropylene Random Copolymer RA130E-2492 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is dark blue colored. Applications: domestic water, heating, relining, plumbing, and in.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis RA130E-6020 Polypropylene Random Copolymer RA130E-6020 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis RA130E-8427 Polypropylene Random Copolymer RA130E-8427 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is grey colored. Applications: domestic water, heating, relining, plumbing, and industr.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® K240-HP Impact Modified Nylon 6 (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, Conditioned Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, Conditioned Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Conditioned (2.5% Moisture) Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Conditioned, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, Conditioned Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -40.0 °C |
9.52 ft-lb/in² @Temperature -40.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**) Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PP HJ752 UV2 Polypropylene/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A ERV3012 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Styrolution Luran® S KR 2861/1 C Colored ASA+PC Description: Grade with high heat resistance for injection molding and extrusion.Applications: Interior and exterior automotive parts, and electrical housings.Information provided by STYROLUTION, wh.. |