Polymer Property : Tensile Modulus = 11.3 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 11.3 GPa
1640 ksi
Plastcom SLOVAMID 66 GF 35 HTS PA66, 355% glass fibre, combined stability
FeaturesPA 66 for injection moulding, chemically reinforced with 35% glass fibre, heat stabilized and stabilized against hydrolysis. Used for cooling water systems in the automotive industry. Delive..
Tensile Modulus 11.3 GPa
1640 ksi
5 mm/min; ASTM D638
LNP NORYL® EXCP0111 PPS + Polyphenylene Ether, 42% Glass / Mineral Reinforcement  (discontinued **)
For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele..
Tensile Modulus 11.3 GPa

@Temperature 23.0 °C
1640 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Rynite® FR530L BK507 PET  (Unverified Data**)
Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Tensile Modulus 11.3 GPa
1640 ksi
ISO 527
Nilit FRIANYL A63 V0 G5 Nylon 6.6 for injection molding, 25% glass fiber reinforced
Nylon 6.6 for injection molding, flame retardant, free of halogen and phosphorus.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Tensile Modulus 11.3 GPa
1640 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL GFN1740V PPE+PS
Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
Tensile Modulus 11.3 GPa
1640 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Asia Pacific)
Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
Tensile Modulus 11.3 GPa
1640 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Europe-Africa-Middle East)
Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
Tensile Modulus 11.3 GPa
1640 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON MV00ASXC PP (Europe-Africa-Middle East)
LNP* VERTON* MV00ASXC is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized.
Tensile Modulus 11.3 GPa
1640 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL EXNL1285 PPE+PS (Europe-Africa-Middle East)
Noryl* EXNL1285 Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
Tensile Modulus 11.3 GPa
1640 ksi
ASTM D638
Plenco 3597 Phenolic, Granular, Injection Molded
PLENCO 03597 is a mineral filled phenolic molding compound offering excellent flammability ratings even at thin cross sections, along with excellent arc and comparative track resistance values. UL r..
Tensile Modulus 11.3 GPa
1640 ksi
ASTM D638
Plenco 4504 Phenolic, Granular, Compression Molded
Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding c..
Tensile Modulus 11.3 GPa
1640 ksi
dry; ISO 527-1/-2
DSM Akulon® N24-G7 PA6-GF35
35% Glass Reinforced
Tensile Modulus 11.3 GPa
1640 ksi
ISO 527-1/-2
DuPont Performance Polymers Rynite® FR530 BK507 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont ..
Tensile Modulus 11.3 GPa
1640 ksi
50%RH; ISO 527-1/-2
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)
30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Improved Flow Zytel HTNFR52G30NHF BK337 is a 30% glass reinforced flame retardant lubricated high performance..
Tensile Modulus 11.3 GPa
1640 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® PLS 95G40DH1T BK261 Nylon 6  (Unverified Data**)
40% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G40DH1T is a 40% GR impact modified PA made with SHIELD technology its superior heatInformation provided by DuPont Performance Polymers
Tensile Modulus 11.3 GPa
1640 ksi
ISO 527
Azoty Tarnow™ TARNOFORM 300 GF7 POM
35% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A...
Tensile Modulus 11.3 GPa
1640 ksi
ISO 527
BASF Ultramid® 66 H2 G/35-V0KB NAT 0046 35% Glass Filled PA66 (Dry)
Description: Ultramid 66 H2 G/35-V0KB NAT0046 is a 35% glass reinforced, heat stabilized injection molding grade. It is a V-0 self-extinguishing grade, with phosphorous. It offers good flowability a..
Tensile Modulus 11.3 GPa
1640 ksi
ISO 527-2
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, Conditioned
Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass..
Tensile Modulus 11.3 GPa
1640 ksi
ISO 527-2
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, Conditioned
Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. ..
Tensile Modulus 11.3 GPa
1640 ksi
ISO 527-2
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, Conditioned
Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, ..
Tensile Modulus 11.3 GPa
1640 ksi
ISO 527-2
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, Conditioned
Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe..
Tensile Modulus 11.3 GPa
1640 ksi
ISO 527-2
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, Conditioned
Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. ..
Tensile Modulus 11.3 GPa
1640 ksi
ISO 527-2
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Conditioned (2.5% Moisture)
Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. ..
Tensile Modulus 11.3 GPa
1640 ksi
ISO 527-1/-2
DuPont Performance Polymers Rynite® FR530L BK507 Polyethylene Terephthalate (PET)
Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Tensile Modulus 11.3 GPa
1640 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL FE1740PW PPE+PS (Europe-Africa-Middle East)
Noryl* FE1740PW Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..