Asahi Kasei Thermylene® P6-30FM-0378 30% Glass/Mineral Reinforced, Heat Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Glass/Mineral Reinforced
Manufacturer Asahi Kasei
Trade Name Thermylene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermylene® P6-30FM-0378 30% Glass/Mineral Reinforced, Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
ASTM D785
Tensile Strength, Yield 70.3 MPa
10200 psi
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Tensile Modulus 4.69 GPa
680 ksi
ASTM D638
Flexural Strength 93.8 MPa
13600 psi
ASTM D790
Flexural Modulus 4.00 GPa
580 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.27 J/cm
8.00 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 158 °C
317 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 143 °C
290 °F
ASTM D648
Flame Spread 30 mm/min
1.2 in/min
Horizontal Burn Rate; FMVSS302