Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 70.3 MPa | 10200 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ PPH-40G Black Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 70.3 MPa | 10200 psi | ASTM D638 |
Polymer Resources PPX-FR6 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 300F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Tensile Strength, Yield | 70.3 MPa | 10200 psi | ASTM D638 |
PTS Trilac® ABS-GF3000-BK 30% Fiberglass Black ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 70.3 MPa | 10200 psi | Clear Casting |
TSE Industries EcoSPRAY® SS100 Aliphatic Polyurethane Resin TSE-EcoSPRAY® SS100 is an “Environmentally-Preferred Product” or EPP. It is an Aliphatic polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during application. TSE-EcoSPRA.. |
|||
Tensile Strength, Yield | 70.3 MPa | 10200 psi | ASTM D638 |
LG Chemical Lupox® PBT-GP-2306FA 30% GFR Flame Retardant, UV Stabilized PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 70.3 MPa | 10200 psi | ASTM D638 |
Techmer ES Electrablend® PC SS10 10% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: ConductiveInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 70.3 MPa | 10200 psi | ASTM D638 |
Techmer ES Statiblend® PC FR BK Availability: North AmericaForms: PelletsAntistaticFeatures: Flame Retardant and Semi ConductiveUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 70.3 MPa | 10200 psi | ASTM D638 |
PlastxWorld Veroplas PB2002 Nylon 66 impact modified, unfilled injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 70.3 MPa | 10200 psi | Clear Casting |
TSE Industries EcoSPRAY® SS100 Aliphatic Polyurethane Resin TSE-EcoSPRAY® SS100 is an “Environmentally-Preferred Product” or EPP. It is an Aliphatic polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during application. TSE-EcoSPRA.. |
|||
Tensile Strength, Yield | 70.3 MPa @Thickness 3.18 mm |
10200 psi @Thickness 0.125 in |
6 mm/min; ASTM D638 |
Chi Mei Acryrex® CM-205 PMMA High heat injection grade. It can resist high temperature. High mechanical strength.Applications: The indicator cover of scooter and automobile/sun glasses/digital watch cover.Features:Good Weather .. |
|||
Tensile Strength, Yield | 70.3 MPa | 10200 psi | ASTM D638 |
Clariant 6602-L BK-02 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 70.3 MPa | 10200 psi | ASTM D638 |
Clariant BRU2000 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 70.3 MPa | 10200 psi | ASTM D638 |
Clariant Renol BRU0000BN-182 Nylon 66, Lubricated, Nucleated, Weather Resistant Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 70.3 MPa | 10200 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-30FM-0378 30% Glass/Mineral Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 70.3 MPa | 10200 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PF-1000 Polysulfone
(discontinued **) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |