Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon R37208T017 0.017" (0.432 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Liner

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon R37208T017 0.017" (0.432 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Liner.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Liner: PTFE Coated Fiberglass Side 1: Uncured Silicone Rubber Substrate: Laminated Tefzel® Substrate: Treated for adhesionThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Silicone Property; Arlon SQA-TMS-024
1.70 g/cc
0.0614 lb/in³
Substrate Property; Arlon SQA-TMS-024
Thickness 50.8 microns
2.00 mil
Substrate; Arlon SQA-TMS-003
76.2 microns
3.00 mil
Liner
381 microns
15.0 mil
Side 1; Arlon SQA-TMS-003
432 microns
17.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 18
18
Silicone Property; ASTM D2240
67
67
Substrate Property; ASTM D2240
Tensile Strength 6.89 MPa
1000 psi
Silicone Property; ASTM D412
41.4 MPa
6000 psi
Substrate Property; ASTM D412
Elongation at Break 300 %
300 %
Substrate Property; ASTM D412
950 %
950 %
Silicone Property; ASTM D412
Modulus of Elasticity 0.000517 GPa
0.0750 ksi
Silicone Property; ASTM E 831
Poissons Ratio 0.50
0.50
Approximately, Silicone Property
Thermal Properties Metric English Comments
CTE, linear 335 µm/m-°C
186 µin/in-°F
Silicone Property; ASTM E 831
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Silicone Property; ASTM E 1530
Maximum Service Temperature, Air 154 °C
310 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 31.1 kV/mm
790 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 15.0 min

@Pressure 0.103 - 0.345 MPa,
Temperature 121 °C
0.250 hour

@Pressure 15.0 - 50.0 psi,
Temperature 250 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 4.44 - 10.0 °C
6.00 Month

@Temperature 40.0 - 50.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Translucent
Total Product Weight (oz/yd2) 14.9
Arlon SQA-TMS-025
Users viewing this material also viewed the following: