Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 432 microns | 17.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 26122P020 0.020" Cured Silicone Rubber/Laminated PTFE Film Design/Construction:Interleave: 0.002" ETFESide 1: Cured Silicone RubberLaminated Substrate: Cast PTFE FilmThis data represents typical values for the production material and should not be used a.. |
|||
Thickness | 432 microns | 17.0 mil | Side 1 |
Arlon 51570R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to wri.. |
|||
Thickness | 432 microns | 17.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 51866R015 0.0170" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Thickness | 432 microns | 17.0 mil | overall; Arlon SQA-TMS-003 |
Arlon 51976XA015 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Thickness | 432 microns | 17.0 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 55146R040 0.040"(1.02 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red sil.. |
|||
Thickness | 432 microns | 17.0 mil | Prime Coated 1564 Fiberglass, Substrate |
Arlon 56590R026 0.026" (0.660 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis data Represents typical values fo.. |
|||
Thickness | 432 microns | 17.0 mil | Prime Coated 1564 Fiberglass, Substrate |
Arlon 56596R045 0.045" (1.14 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silicone gum and rubber on fiberglass with polymer release lin.. |
|||
Thickness | 432 microns | 17.0 mil | Prime Coated 1564 Fiberglass, Substrate |
Arlon 56596R065 0.065" (1.65 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silicone gum and rubber on fiberglass with polymer release li.. |
|||
Thickness | 432 - 584 microns | 17.0 - 23.0 mil | Overall |
Arlon 920-20Bxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 2Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i.. |
|||
Thickness | 432 - 584 microns | 17.0 - 23.0 mil | Overall |
Arlon 920-20Txx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 2Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i.. |
|||
Thickness | 432 - 584 microns | 17.0 - 23.0 mil | Overall |
Arlon LW202Bxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Thickness | 432 microns | 17.0 mil | Tape |
3M Cushion-Mount™ 1015 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Thickness | 432 microns | 17.0 mil | Tape |
3M Cushion-Mount™ 1815M Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Thickness | 432 - 559 microns | 17.0 - 22.0 mil | Side 1 |
Arlon R30651R062 0.062" (1.57 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 432 - 559 microns | 17.0 - 22.0 mil | Side 2 |
Arlon R30651R062 0.062" (1.57 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 432 microns | 17.0 mil | Tape |
3M Cushion-Mount™ E1015 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 432 microns | 17.0 mil | Tape |
3M Cushion-Mount™ E1115 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 432 microns | 17.0 mil | Tape |
3M Cushion-Mount™ E1215 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 432 microns | 17.0 mil | Tape |
3M Cushion-Mount™ E1315 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 432 microns | 17.0 mil | Tape |
3M Cushion-Mount™ E1515 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 432 microns | 17.0 mil | Tape |
3M Cushion-Mount™ E1715 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 432 microns | 17.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 51344R025 0.025" (0.635 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Semi-Cured Silicone RubberSubstrate: Style 7628 FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values fo.. |
|||
Thickness | 432 microns | 17.0 mil | Prime Coated 1564 Fiberglass, Substrate |
Arlon 56224R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info.. |
|||
Thickness | 432 microns | 17.0 mil | Tape; ASTM D3652 |
3M 9343 Conformable Sound Management Film 3M™ Conformable Sound Management Film 9343 is designed for the reduction of noise, vibration, squeaks, and rattles in automotive interior applications. The currently available materials for these a.. |
|||
Thickness | 432 microns | 17.0 mil | Tape |
3M Cushion-Mount™ 1115 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Thickness | 432 microns | 17.0 mil | Tape |
3M Cushion-Mount™ E1815 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 432 microns | 17.0 mil | Tape |
3M Cushion-Mount™ E1915 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 432 microns | 17.0 mil | Tape |
3M Cushion-Mount™ 1915M Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Thickness | 432 microns | 17.0 mil | Tape |
3M Cushion-Mount™ E1920 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |