Modulus of Elasticity 0.000517 - 1.90 GPa
0.0750 - 276 ksi
Average value: 0.0881 GPa Grade Count:27
Overview of materials for Silicone Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma..
Modulus of Elasticity 0.000517 GPa
0.0750 ksi
Silicone Property; ASTM E 831
Arlon R36798T017 0.017" (0.432 mm) Uncured Silicone Rubber with Laminated Tefzel® Substrate  (discontinue
Design/Construction: Liner: PTFE Coated Fiberglass Side 1: Uncured Silicone Rubber Substrate: Laminated Tefzel® Substrate: Treated for adhesionAppearance: Translucent, high viscosity gum on fluoro..
Modulus of Elasticity 0.000517 GPa
0.0750 ksi
Arlon SQA-TMS-008
Arlon 25188T010 Silicone Rubber/Laminated ETFE Film
Liner: 3 mil PTFE coated fiberglass; Side 1: uncured silicone rubber; Substrate: laminated ETFE film, treated for adhesion
Modulus of Elasticity 0.000517 GPa
0.0750 ksi
Arlon SQA-TMS-008
Arlon 25188T017 Silicone Rubber/Laminated ETFE Film
Liner: 3 mil PTFE coated fiberglass; Side 1: uncured silicone rubber; Substrate: laminated ETFE film, treated for adhesion
Modulus of Elasticity 0.000517 GPa
0.0750 ksi
Silicone Property; ASTM E 831
Arlon R37208T017 0.017" (0.432 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Liner
Design/Construction: Liner: PTFE Coated Fiberglass Side 1: Uncured Silicone Rubber Substrate: Laminated Tefzel® Substrate: Treated for adhesionThis data represents typical values for the productio..
Modulus of Elasticity 0.000517 GPa
0.0750 ksi
Silicone Property; ASTM E 831
Arlon R37230R006 0.006" (0.152 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Substrate
Design/Construction: Liner: FEP Add-on: Uncured Silicone Rubber Substrate: PTFE Coated Fiberglass This data represents typical values for the production material. The data should not be used to wri..
Modulus of Elasticity 0.000517 GPa
0.0750 ksi
silicone property; Arlon SQA-TMS-008
Arlon Thermabond® 99180T010 Silicone Rubber/Fiberglass Laminate
Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.