Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
Polykemi AB POLYshine PBT D204 GF30 FR PBT, Glass Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | |
IDI Composites 46-16-60 Thermoset Polyester, Sheet TRANSIT - A premium molding compound with excellent resistance to flame and smoke generation, high impact strength, and weatherability.Data provided by the manufacturer. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | |
IDI Composites C-206 Thermoset Polyester, Sheet CORROSION - (Patent pending). Versatile family of compounds designed for pressurized and thermo-mechanically stressed applications. Excellent corrosion resistance and high strength.Data provided by .. |
|||
Density | 1.70 - 1.90 g/cc | 0.0614 - 0.0686 lb/in³ | theoretical |
Gwent Electronic Materials P2121112P11 Oxygen Plasma Modified Multiwalled Carbon Nanotubes Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Density | 1.70 - 1.90 g/cc | 0.0614 - 0.0686 lb/in³ | theoretical |
Gwent Electronic Materials P2121112P13 Argon Plasma Modified Single and Double Walled Carbon Nanotubes Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Density | 1.70 - 1.90 g/cc | 0.0614 - 0.0686 lb/in³ | theoretical |
Gwent Electronic Materials P2121112P7 Acid Vapor Plasma Modified Multiwalled Carbon Nanotubes Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
Lanxess Pocan® DP 7244 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D572 |
Haysite 30000 Polyester BMC, 15% Glass Reinforced Haysite 30000 series bulk molding compound is a general purpose material. This compound can be compression, transfer, or injection molded. This material has good mechanical properties and can be pig.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
Menzolit Menzolit® SMC 0300 Unsaturated Polyester UP SMC 0300 is a low shrink standard SMC providing improved surface quality, reduced shrinkage and warpage. Typical fields of applications are mechanical engineering and electrical industry, where impr.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing 30% Glass Fiber, 15% PTFE. Added featurs of this material is: Wear Resistant. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES (Asia Pacific) LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF60 HS L BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackProcessing Method: In.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF60 HS L BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 LGF60 HS L BK 12 mm Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass FiberAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Heat Stabilized and Good MoldabilityAppearance: BlackProce.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | GB/T 1033.1-2008 |
Sichuan Deyang Haton® hGR515 Polyphenylene Sulfide/PA Alloy Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | |
Sawbones E-Glass-Filled Epoxy Sheets Primary UseE-glass-filled epoxy sheets are primarily used as an alternative test medium to human cortical bone.DescriptionE-glass-filled epoxy sheets are a mixture of short e-glass fibers and epoxy .. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | |
Sawbones Third-Generation Simulated Cortical Bone E-glass-filled EpoxySawbones® Third-Generation Bones model natural cortical bone using a mixture of short e-glass fibers and epoxy resin pressure injected around a foam core. The mid-shaft area h.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® V8280SF PBT+PET High Modulus, PBT+PET, 40% Glass Reinforced, Mold Release, Super High Flow |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | |
Sawbones E-Glass-Filled Epoxy Cylinders Primary UseE-glass-filled epoxy cylinders are primarily used as an alternative test medium to human cortical bone.DescriptionThey are a mixture of short e-glass fibers and epoxy resin that has been .. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
Unitika A1022GFL60 PA6, 60% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | Relative Density; ISO 1183 |
Vyncolit X681 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction. Tribological compound with PTFE additive.USES: Water pump seals and self-lubrica.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | |
Zircar Refractory Composites RS-99M Refractory Sheet Type RS-99M is a plastic highly moldable sheet ideally suited for forming custom geometries.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI) |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | |
Loctite® 3151 1 component acrylic UV/Heat Cure Acrylic Adhesive Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 |
Ensinger Tecatron® XP-64 Compression Molded PPS Compound, 40% Fiberglass Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 |
Ensinger Tecatron® XP-65 Compression Molded PPS Compound, 30% Fiberglass with 15% PTFE Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon Thermabond® R36300W008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Low Outgassing, Thermally Conductive, Electrically Insulating, Thermabond® Bonds without primerRecommended Primers: Dow Corning S2260Design/Construction: Liner: FEP Product: Uncured S.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | |
A. Schulman ComAlloy Voloy® 430 Glass Reinforced, PBT Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 |
Plenco 1506 Polyester, Briquette, Injection Molded PLENCO 01506 is a mineral and cellulose filled granular polyester molding compound, with glass fiber reinforcement for improved mechanical strength properties. 01506 offers excellent electrical prop.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
Hexion Bakelite™ PF 4010 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage
(disconti Glass fiber reinforced and inorganically filled molding compound. High heat resistance, reduced molding shrinkage, good chemical resistance and mechanical properties.Application areas: Switch housi.. |