Polymer Property : Density = 1.70 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.70 - 1.73 g/cc
0.0614 - 0.0625 lb/in³
Liquid
Oceanchem Group Calcium Bromide (CaBr2)
Molecular Formula: CaBr2Cas No.: 7789-41-5Use: Calcium Bromide and its formuulated brines are mainly used as completion, workover and packer fluids in oil drilling field.Properties: This product is ..
Density 1.70 g/cc
0.0614 lb/in³
Pyrotek Pyroboard™ S400 Roller
Pyroboard™ S400 is a low temperature material that is normally used in cooling zones where water quenching is present.Information provided by Pyrotek.
Density 1.70 - 1.90 g/cc
0.0614 - 0.0686 lb/in³
Average value: 1.78 g/cc Grade Count:6
Overview of materials for Phenolic, Resole, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
Density 1.70 g/cc
0.0614 lb/in³
ISO 1183
Menzolit Menzolit® SMC 0200 Unsaturated Polyester UP
SMC 0200 is a general purpose SMC for a wide range of applications. Typically, it is used as housings, covers and functional components in mechanical engineering. The flammability meets the demands ..
Density 1.70 g/cc
0.0614 lb/in³
ISO 1183
Menzolit Menzolit® SMC 1000 Unsaturated Polyester UP
SMC 1000 is a special SMC for hydrolysis resistant applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Typical applications are ..
Density 1.70 g/cc
0.0614 lb/in³
ISO 1183
Menzolit Menzolit® SMC 1650 Unsaturated Polyester UP
SMC 1650 is a specially designed anti-microbial polyester moulding compound which incorporates a "germ killer" . It has been tested and found to be compliant for resistance to fungal defacement in ..
Density 1.70 - 1.90 g/cc
0.0614 - 0.0686 lb/in³
theoretical
Gwent Electronic Materials P2121112P13 Argon Plasma Modified Single and Double Walled Carbon Nanotubes
Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Density 1.70 g/cc
0.0614 lb/in³
ISO 1183
Menzolit Menzolit® SMC 0290 Unsaturated Polyester UP
SMC 0290 is a specially formulated SMC processable by injection moulding. The gentle production process prevents the fiber from any damage. Parts made of SMC 0290 reach higher levels of strength and..
Density 1.70 g/cc
0.0614 lb/in³
ISO 1183
SABIC Innovative Plastics LNP LUBRICOMP WFL28 PBT (Europe-Africa-Middle East)
LNP* LUBRICOMP* WFL28 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated.
Density 1.70 g/cc
0.0614 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON RX05488 PA 66
LNP STAT-KON* RX05488 is a compound based on Nylon 66 resin containing Carbon Fiber, Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Electrically Conductive.
Density 1.70 g/cc
0.0614 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP OF008H PPS - Linear
LNP* THERMOCOMP* OF008H is a compound based on PPS - Linear containing 40% Glass Fiber. Characteristics of this grade are: Healthcare.
Density 1.70 g/cc
0.0614 lb/in³
ASTM D792
Techmer ES HiFill FR® PA6/6 GF40 FR HS L 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInform..
Density 1.70 g/cc
0.0614 lb/in³
ASTM D792
Techmer ES Luriblend® PES GF30 TL15 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: LubricatedInformation provided by TP Composites, Inc.
Density 1.70 g/cc
0.0614 lb/in³
ASTM F1315
Thermoseal KLINGERSIL® C-8200 Chemical Resistant Gasketing
Synthetic FiberHypalon® BinderAcid ResistantGood Oil-Fuel ResistanceGood Gas SealabilityNo Color AddedInformation provided by Thermoseal Inc.
Density 1.70 g/cc
0.0614 lb/in³
Relative Density; ISO 1183
Vyncolit X681 Novolac Phenolic
Glass fiber filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction. Tribological compound with PTFE additive.USES: Water pump seals and self-lubrica..
Density 1.70 - 1.86 g/cc
0.0614 - 0.0672 lb/in³
ASTM D792
Zeus ETFE Tubing
ETFE (Ethylenetetrafluoroethylene), a copolymer of ethylene and tetrafluoroethylene, is used in applications requiring excellent impact, abrasion and stress cracking resistance. This polymer possess..
Density 1.70 g/cc
0.0614 lb/in³
Relative Density; ISO 1183
Vyncolit 2723 W Novolac Phenolic
Mineral and organic filled phenolic molding compound with excellent mechanical, thermal and dielectric properties. I2/FO classified under NF F 16-101 (Fire & Smoke classification).USES: Circuit bre..
Density 1.70 g/cc
0.0614 lb/in³
Relative Density; ISO 1183
Vyncolit 2950 W Novolac Phenolic
Mineral and glass fiber filled phenolic molding compound with a very high strain to failure in flexure. UL listed.USES: Armature insulation.Information provided by Vyncolit, a Sumitomo Bak Group
Density 1.70 g/cc
0.0614 lb/in³
Loctite® Output™ 315 Acrylic Adhesive
Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or..
Density 1.70 g/cc
0.0614 lb/in³
ISO 1183
EMS-Grivory Grivory® LVX-65H SST nat PA12-GF65
Product description: Grilamid LVX-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following pro..
Density 1.70 g/cc
0.0614 lb/in³
ISO 1183
Eurotec® Tecodur® PB70 GR50 NL PBT 50% glass fiber reinforced
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
Density 1.70 g/cc
0.0614 lb/in³
ISO 1183
Akro-Plastic Akromid® B3 GF 60 (2476) PA 6 Conditioned, 60% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Density 1.70 g/cc
0.0614 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon Thermabond® R36300W015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Corning S2260Appearance: White silicone gumThis data represents typical val..
Density 1.70 g/cc
0.0614 lb/in³
cured; ASTM D794
3M Scotchcast™ 5555 10G Electrical Insulating Epoxy Resin
3M Scotchcast Electrical Resin 5555 is a one-part, green pigmented, rapid heat curing powder coating. It is designed to provide a continuous, tough moisture and chemical resistant dielectric coating..
Density 1.70 - 1.80 g/cc
0.0614 - 0.0650 lb/in³
Molding; IS 867-1963
Amity Thermosets ATO 159 Phenolic Molding Glass/ inorganic Filler, Compression Molded
Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit..
Density 1.70 g/cc
0.0614 lb/in³
ISO 1183
DSM Arnite® TV4 264 SN PBT-GF30 FR(17)
30% Glass Reinforced, Flame Retardant
Density 1.70 g/cc
0.0614 lb/in³
Relative Density; ISO 1183
Vyncolit X682 Novolac Phenolic
Glass fiber, glass bead and graphite filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction.USES: Water pump seals and self-lubricating bearings.Info..
Density 1.70 g/cc
0.0614 lb/in³
ISO 1183
Hexion Bakelite™ PF 4010 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage  (disconti
Glass fiber reinforced and inorganically filled molding compound. High heat resistance, reduced molding shrinkage, good chemical resistance and mechanical properties.Application areas: Switch housi..
Density 1.70 g/cc
0.0614 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Verton WV00A PBT (Europe-Africa-Middle East)
LNP VERTON* WV00A is a compound based on Polybutylene Terephalate resin containing Long Glass.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.