Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 154 °C | 309 °F | Continuous |
Pyrotek TS-125 Thermoset Electrical Insulation Product Glass reinforcement, Polyester Resin, Brown Color. Very high mechanical strength at room and elevated temperature. Flame retardant.Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 154 °C | 310 °F | |
Arlon R36798T017 0.017" (0.432 mm) Uncured Silicone Rubber with Laminated Tefzel® Substrate
(discontinue Design/Construction: Liner: PTFE Coated Fiberglass Side 1: Uncured Silicone Rubber Substrate: Laminated Tefzel® Substrate: Treated for adhesionAppearance: Translucent, high viscosity gum on fluoro.. |
|||
Maximum Service Temperature, Air | 154 °C | 310 °F | |
Saint-Gobain CHR® C680 Paper Backing Silicone Adhesive Pressure Sensitive Tape Description: Paper tapes are designed to provide high temperature and excellent solvent resistance for wave soldering, printed circuit board masking, and hot air leveling applications. Service tempe.. |
|||
Maximum Service Temperature, Air | 154 °C | 310 °F | |
Techmer ES HiFill® TPX-HTN-01033 A 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthUL File .. |
|||
Maximum Service Temperature, Air | 154 °C | 310 °F | Continuous Use |
Westlake Plastics Tefzel® 2181 ETFE Products made from Tefzel® HT-2181 resin are suitable for a variety of processes and demanding end uses. They are mechanically tough and offer an excellent balance of properties. These products p.. |
|||
Maximum Service Temperature, Air | 154 °C | 310 °F | |
Arlon 25188T010 Silicone Rubber/Laminated ETFE Film Liner: 3 mil PTFE coated fiberglass; Side 1: uncured silicone rubber; Substrate: laminated ETFE film, treated for adhesion |
|||
Maximum Service Temperature, Air | 154 °C | 310 °F | |
Arlon 25188T017 Silicone Rubber/Laminated ETFE Film Liner: 3 mil PTFE coated fiberglass; Side 1: uncured silicone rubber; Substrate: laminated ETFE film, treated for adhesion |
|||
Maximum Service Temperature, Air | 154 °C | 310 °F | |
Arlon 25662T010 0.010" (0.254 mm) Cured Silicone Rubber with Laminated ETFE Film Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Laminated ETFE FilmChemical Compatibility: (ETFE offers good chemical resistance to the following classes of chemicals) Alkalis, Organic a.. |
|||
Maximum Service Temperature, Air | 154 °C | 310 °F | |
Arlon R37208T017 0.017" (0.432 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Liner Design/Construction: Liner: PTFE Coated Fiberglass Side 1: Uncured Silicone Rubber Substrate: Laminated Tefzel® Substrate: Treated for adhesionThis data represents typical values for the productio.. |