Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 55576R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 55576R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Uncured Silicone Rubber Interleave: LDPE This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Side 2, Silicone Property; Arlon SQA-TMS-024
1.33 g/cc
0.0480 lb/in³
Side 1, Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Side 1; Arlon SQA-TMS-003
76.2 microns
3.00 mil
Interleave
229 microns
9.00 mil
Side 2; Arlon SQA-TMS-003
457 microns
18.0 mil
Substrate; Arlon SQA-TMS-003
762 microns
30.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 36
36
Side 2, Silicone Property; ASTM D2240
50
50
Side 1, Silicone Property; ASTM D2240
Tensile Strength 5.34 MPa
775 psi
Side 1, Silicone Property; ASTM D412
6.38 MPa
925 psi
Side 2, Silicone Property; ASTM D412
Elongation at Break 325 %
325 %
Side 1, Silicone Property; ASTM D412
550 %
550 %
Side 2, Silicone Property; ASTM D412
Tear Strength 8.77 kN/m
50.0 pli
Side 1, Silicone Property; ASTM D624
14.5 kN/m
83.0 pli
Side 2, Silicone Property; ASTM D624
Peel Strength 4.38 kN/m
25.0 pli
Bond Strength; ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 16.7 kV/mm
425 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 177 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 350 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 28.5
Arlon SQA-TMS-025