Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 6.38 MPa | 925 psi | Silicone Property; ASTM D412 |
Arlon 4570XB025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)< Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1165 Fiberglass This data represents typical values for the production material. The data should not be .. |
|||
Tensile Strength | >= 6.37 MPa | >= 925 psi | ASTM D 638 |
Karina 550D02/101-AT-IS Yellow PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 6.37 MPa | >= 925 psi | ASTM D 638 |
Karina 550D02/101-AT-IS Yellow PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 6.37 MPa | >= 925 psi | ASTM D 638 |
Karina E 602D06/719-A-AT-IS Blue PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 6.37 MPa | >= 925 psi | ASTM D 638 |
Karina E 700-08/166-B Beige PVC Compound For footware/soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | 6.38 MPa | 925 psi | |
Teknor Apex Tekbond® TB 1176A Thermoplastic Elastomer Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b.. |
|||
Tensile Strength | 6.38 MPa | 925 psi | Silicone Property; ASTM D412 |
Arlon 32570R040 0.040" (1.02 mm) Uncured Silicone Rubber with Fiberglass Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PTFE Coated FiberglassThis data represents typical values for the production material. The data should not be use.. |
|||
Tensile Strength | 6.38 MPa | 925 psi | Silicone Property; ASTM D412 |
Arlon 51576XC015A 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Cured Silicone Rubber This data represents typical values for the production mat.. |
|||
Tensile Strength | 6.38 MPa | 925 psi | Silicone Property; ASTM D412 |
Arlon 51576XC15A 0.015" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 2: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the producti.. |
|||
Tensile Strength | 6.38 MPa | 925 psi | Side 2, Silicone Property; ASTM D412 |
Arlon 55576R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Uncured Silicone Rubber Interleave: LDPE This data represents typical values for the production material. T.. |
|||
Tensile Strength | 6.38 MPa | 925 psi | Silicone Property; ASTM D412 |
Arlon CP-410R Bulk Compound Design/Construction: Bulk Compound (packaged in polyethylene) This data Represents typical values for the production material. The data should not be used to write, or in place of, material specific.. |
|||
Tensile Strength | 6.38 MPa | 925 psi | Silicone Property; ASTM D412 |
Arlon CP-410XD Bulk Compound Design/Construction:Bulk Compound (packaged in polyethylene) This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifica.. |
|||
Tensile Strength | 6.38 MPa | 925 psi | Silicone Property; ASTM D412 |
Arlon 44576R009A 0.0058" (0.216 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 1165 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production ma.. |
|||
Tensile Strength | 6.38 MPa | 925 psi | Silicone Property; ASTM D412 |
Arlon 44570XB025 0.025" Uncured Silicone Rubber with Fiberglass Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 FiberglassThis data represents typical values for the production material and should not b.. |