Arkema Group Rilsan® BESN TL Nylon 11, Rigid Tubing Grade (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11, Unreinforced
Manufacturer Arkema
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® BESN TL Nylon 11, Rigid Tubing Grade (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation ISO 1874-PA11,EHL,22-010Rigid grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Good chemical resistance. Ability to be processed at high speed. Easy to color (sublimation).Example applications: Pneumatic suspension line.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
Water Absorption 1.9 %
1.9 %
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 235 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.0 MPa
5950 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 6.0 %
6.0 %
50 mm/min
Tensile Modulus 1.47 GPa
213 ksi
1 mm/min
Thermal Properties Metric English Comments
Melting Point 183 °C
361 °F
10°C/min
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
V-2

@Thickness 3.20 mm
V-2

@Thickness 0.126 in
Oxygen Index 25 %
25 %
Electrical Properties Metric English Comments
Dissipation Factor 0.000328

@Frequency 1e+6 Hz
0.000328

@Frequency 1e+6 Hz
0.000333

@Frequency 100 Hz
0.000333

@Frequency 100 Hz