Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 518581R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. Th.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Side 1 |
Arlon 15370T020 0.020" (0.508 mm) Uncatalyzed, Unsupported Rubber on a Mylar Carrier Design/Construction:Side 1: Uncatalyzed, Unsupported Rubber on a Mylar CarrierAppearance: Translucent high viscosity gumThis data represents typical values for the production material. The data shou.. |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Fiberglass, Substrate |
Arlon 55191R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. Th.. |
|||
Thickness | 457 microns | 18.0 mil | Style 162 Fiberglass, Substrate; Arlon SQA-TMS-003 |
Arlon 55572XD028 0.028" (0.711 mm) Cured Silicone Rubber Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Thickness | 457 microns | 18.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55576R060 0.060" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Thickness | 457 microns | 18.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55579R055 0.054" (1.37 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum and rubber on fiberglass clot.. |
|||
Thickness | 457 microns | 18.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55586R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneAppearance: Red silicone gum and rubber on fiberglass clothTh.. |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Fiberglass, Substrate |
Arlon 55596R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Fiberglass, Substrate |
Arlon 55609R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThi.. |
|||
Thickness | 457 microns | 18.0 mil | substrate; Arlon SQA-TMS-003 |
Arlon 55946C028 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 162 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Fiberglass, Substrate |
Arlon 55949C028W 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in pl.. |
|||
Thickness | 457 microns | 18.0 mil | Substrate |
Arlon 56606R026 0.027" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production materia.. |
|||
Thickness | 457 microns | 18.0 mil | Substrate |
Arlon 56609R028 0.029" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassThis data represents typical values for the production materi.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 920-07Rxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tap.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon LW201Xxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Thickness | 457 microns | 18.0 mil | Side 2; Arlon SQA-TMS-003 |
Arlon R39091R036 0.036" (0.914 mm) Uncured Silicone Rubber with Nomex Fabric Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1574 Nomex FabricSide 2: Uncured SiliconeInterleave: Polyethylene This data represents typical values fo.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 51268R020P 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Silicone RubberThickness:Side 1: Skim CoatSide 2: Skim Coat + 0.010" uncuredThis data Represents typical values for the product.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 51420R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info.. |
|||
Thickness | 457 microns | 18.0 mil | substrate; Arlon SQA-TMS-003 |
Arlon 55143R060 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 2: cured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber |
|||
Thickness | 457 microns | 18.0 mil | Style 162 Fiberglass, Substrate; Arlon SQA-TMS-003 |
Arlon 55273R060 0.060" (1.52 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, .. |
|||
Thickness | 457 microns | 18.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55276B028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Cured Silicone Rubber This data represents typical values for the production mate.. |
|||
Thickness | 457 microns | 18.0 mil | Substrate |
Arlon 55359R062 62 mil Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materi.. |
|||
Thickness | 457 microns | 18.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55560R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for.. |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Fiberglass, Substrate |
Arlon 55949C028 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone Rubber Appearance: Brown silicone rubber and gum on fiberglass clothThis data Represents typical values for the produc.. |
|||
Thickness | 457 microns | 18.0 mil | Side 1 |
Arlon 59463X068CT 0.068" (1.73 mm) Textured, Cured Rubber with Fiberglass Substrate Design/Construction:Side 1: Textured, Cured Rubber Side 2: Textured, Cured Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Fiberglass, Substrate |
Arlon R31551R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place.. |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Style Fiberglass, Substrate |
Arlon R33468A030 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured LayersAppearance: Semi-cured blue silicone gum on glass fabricThis data Represents typical values for the production material. .. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon R33889R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Layer-on-Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information .. |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Style Fiberglass, Substrate |
Arlon R34688XA030 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured/Cured LayersThis data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 44602M020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberAppearance Tan rubber on glass fiber fabricThis data represents typical values for the production material. The data should not be used to write, or .. |