Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 14.5 kN/m | 83.0 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7345-9000 TPE Product Description: StarFlex P 7345-9000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelGood WeatherabilityFDA and medical grades availableProcessing Method.. |
|||
Tear Strength | 14.5 kN/m | 82.7 pli | Die C; ASTM D624 |
Teknor Apex Telcar® TL-6045 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tear Strength | 14.5 kN/m | 83.0 pli | ASTM D624 |
Teknor Apex UNIPRENE® 7100-45 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tear Strength | 14.5 kN/m | 82.7 pli | ASTM D624 |
Teknor Apex Uniprene® UN-1141A Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tear Strength | 14.5 kN/m | 82.7 pli | ASTM D624 |
Teknor Apex Uniprene® UN-7100-45 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tear Strength | 14.5 kN/m | 83.0 pli | Silicone, Die B; ASTM D624 |
Arlon 18976XA023 Silicone Rubber/Fiberglass Laminate Side 1:cured silicone rubber; Substrate: 11523 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil Polyethylene |
|||
Tear Strength | 14.5 kN/m | 83.0 pli | Silicone Property; ASTM D624 |
Arlon 31970XA015 Silicone Rubber Laminate The interleave is 3 mil of polyethylene, side 1 is uncured silicone rubber and the carrier is HDPE. |
|||
Tear Strength | 14.5 kN/m | 83.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon 32570R040 0.040" (1.02 mm) Uncured Silicone Rubber with Fiberglass Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PTFE Coated FiberglassThis data represents typical values for the production material. The data should not be use.. |
|||
Tear Strength | 14.5 kN/m | 83.0 pli | Die B; silicone property; ASTM D624 |
Arlon 51976XA015 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Tear Strength | 14.5 kN/m | 83.0 pli | Die B; Silicone Property; Arlon SQA-TMS-029 |
Arlon 55572GA028 0.028" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production material and should not be used as material .. |
|||
Tear Strength | 14.5 kN/m | 83.0 pli | [ppiw], Die B, Silicone Property; ASTM D624 |
Arlon 55572R030 0.030" (0.762 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. T.. |
|||
Tear Strength | 14.5 kN/m | 83.0 pli | [ppiw], Die B, Silicone Property; ASTM D624 |
Arlon 55572XA028 0.028" (0.711 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Tear Strength | 14.5 kN/m | 83.0 pli | [ppiw], Die B, Silicone Property; ASTM D624 |
Arlon 55572XD028 0.028" (0.711 mm) Cured Silicone Rubber Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Tear Strength | 14.5 kN/m | 83.0 pli | Side 2, Silicone Property; ASTM D624 |
Arlon 55576R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Uncured Silicone Rubber Interleave: LDPE This data represents typical values for the production material. T.. |
|||
Tear Strength | 14.5 kN/m | 83.0 pli | Die B; silicone property; ASTM D624 |
Arlon 56976XA026 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 1564 fiberglass; Side 2: uncured silicone rubber |
|||
Tear Strength | 14.5 kN/m | 83.0 pli | Silicone Property; ASTM D624 |
Arlon 99570R010 0.010" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction:Liner: 0.001" FEP FilmSide 1: Uncured Silicone RubberCarrier: 0.003" PTFE coated FiberglassThis data represents typical values for the production material and should not be us.. |
|||
Tear Strength | 14.5 kN/m | 83.0 pli | Silicone Property; ASTM D624 |
Arlon CP-410R Bulk Compound Design/Construction: Bulk Compound (packaged in polyethylene) This data Represents typical values for the production material. The data should not be used to write, or in place of, material specific.. |
|||
Tear Strength | 14.5 kN/m | 83.0 pli | Silicone Property; ASTM D624 |
Arlon CP-410XD Bulk Compound Design/Construction:Bulk Compound (packaged in polyethylene) This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifica.. |
|||
Tear Strength | 14.5 kN/m | 83.0 pli | [ppiw], Die B, Silicone Property; ASTM D624 |
Arlon 55572R028 0.028" (0.711 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. T.. |
|||
Tear Strength | 14.5 kN/m | 83.0 pli | Die B; Silicone Property; Arlon SQA-TMS-029 |
Arlon 32570XA020 0.020" Uncured Silicone Rubber on Polyester Film Carrier Design/Construction:Interleave: 0.0025" PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as .. |