Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 518581R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. Th.. |
|||
Thickness | 457 microns | 18.0 mil | Gauge, nominal |
Mid-Mountain Materials ARMATEX® SF18 Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 10842S020 0.020" (0.508 mm) Fully Cured, Unsupported, Silicone Rubber Design/Construction:Side 1: Fully Cured, Unsupported, Silicone Rubber Appearance: Dark red silicone rubberThis data represents typical values for the production material. The data should not be used.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 15370T020 0.020" (0.508 mm) Uncatalyzed, Unsupported Rubber on a Mylar Carrier Design/Construction:Side 1: Uncatalyzed, Unsupported Rubber on a Mylar CarrierAppearance: Translucent high viscosity gumThis data represents typical values for the production material. The data shou.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Side 1 |
Arlon 30570R020 0.020" (0.508 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 51582R020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Inform.. |
|||
Thickness | 457 microns | 18.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55572XA028 0.028" (0.711 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Thickness | 457 microns | 18.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55576R060 0.060" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Style Fiberglass, Substrate |
Arlon 55578XD028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers Appearance: Gray silicone gum and/or rubber on fiberglass clothThis data Represents typical values for the production ma.. |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Style Fiberglass, Substrate |
Arlon 55579R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured layer on top of a cured layer on one side Appearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production materi.. |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Style Fiberglass, Substrate |
Arlon 55579R043W 0.043" (1.09 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured layer on top of a cured layer on one side This data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Thickness | 457 microns | 18.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55581R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: 162 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneAppearance: Red silicone gum on.. |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Fiberglass, Substrate |
Arlon 55609R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThi.. |
|||
Thickness | 457 microns | 18.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55900R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: 162 Style Fiberglass Appearance: Red silicone gum on glass fabricThis data represents typical values for the p.. |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Fiberglass, Substrate |
Arlon 55949C028W 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in pl.. |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Fiberglass, Substrate |
Arlon 55978X030 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Cured/Uncured Layers Appearance: Gray silicone gum on glass fiber fabricThis data Represents typical values for the production material.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 920-05Rxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 0.5Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 920-20Bxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 2Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Side 1 |
Arlon 30580R020 0.020" (0.508 mm) Uncured Unsupported Silicone Rubber on Kodacel Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Kodacel CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The da.. |
|||
Thickness | 457 microns | 18.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 51583R018 0.018" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: 2.5 mil LDPESide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave 2: 2.5 mil LDPEThis data represents typical val.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 51971R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red gum on glass fiber fabricThis data Represents typical values for the production material. The data .. |
|||
Thickness | 457 microns | 18.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55271R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Cured Silicone Rubber Interleave 2: Polyethylene Product Use: Flexible heater in.. |
|||
Thickness | 457 microns | 18.0 mil | Substrate |
Arlon 55503R062 0.062" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Prime Coated 162 Style FiberglassSide 2: Cured Silicone RubberThis data represents typical values for th.. |
|||
Thickness | 457 microns | 18.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55580R025 0.026" (0.660 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneRubber Layer: Uncured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values .. |
|||
Thickness | 457 microns | 18.0 mil | Side 1 |
Arlon 59463X068CT 0.068" (1.73 mm) Textured, Cured Rubber with Fiberglass Substrate Design/Construction:Side 1: Textured, Cured Rubber Side 2: Textured, Cured Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Style Fiberglass, Substrate |
Arlon R33468A030 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured LayersAppearance: Semi-cured blue silicone gum on glass fabricThis data Represents typical values for the production material. .. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon R33889R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Layer-on-Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information .. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Side 1 |
Arlon R34880T020 0.020" (0.508 mm) Uncatalyzed, Unsupported rubber on a Mylar Carrier Design/Construction:Side 1: Uncatalyzed, Unsupported rubber on a Mylar Carrier This data Represents typical values for the production material. The data should not be used to write, or in place of, .. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 44602W020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberProduct Use: Flexible heater insulationAppearance: White silicone rubber on fiberglassThis data represents typical values for the production material.. |
|||
Thickness | 457 microns | 18.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 44278R018B 0.018" Uncured/Cured/Uncured Silicone Rubber Laminate with Fiberglass Substrate Design/Construction:Interleave 1: LDPESide 2 Layer 2: Uncured Silicone RubberSide 2 Layer 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassSide 1: Cured Silicone RubberInterleave: LDPEUL R.. |