| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.02 g/cc | 0.0368 lb/in³ | ASTM D792 |
| Water Absorption | 0.90 % | 0.90 % | 24 hr in water at 20°C; ASTM D570 |
| Water Absorption at Saturation | 0.70 % | 0.70 % | 20°C and 65% RH; ASTM D570 |
| Melt Flow | 4.0 g/10 min | 4.0 g/10 min | ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 72 | 72 | ASTM D2240 |
| Tensile Strength at Break | 62.0 MPa | 8990 psi | ASTM D638 |
| Tensile Strength, Yield | 34.0 MPa | 4930 psi | ASTM D638 |
| Elongation at Break | 360 % | 360 % | ASTM D638 |
| Elongation at Yield | 15 % | 15 % | ASTM D638 |
| Flexural Modulus | 0.730 GPa | 106 ksi | ASTM D790 |
| Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256-A |
| 0.750 J/cm <br>@Temperature -40.0 °C |
1.41 ft-lb/in <br>@Temperature -40.0 °F |
ASTM D256-A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Heat of Fusion | 63.0 J/g | 27.1 BTU/lb | ASTM D3417 |
| CTE, linear | 120 µm/m-°C <br>@Temperature -40.0 - 140 °C |
66.7 µin/in-°F <br>@Temperature -40.0 - 284 °F |
ASTM D696 |
| Melting Point | 174 °C | 345 °F | ASTM D3418 |
| Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | ASTM D648 |
| Vicat Softening Point | 165 °C | 329 °F | under 1 daN; ASTM D1525 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 5.00e+13 ohm <br>@Temperature 20.0 °C |
5.00e+13 ohm <br>@Temperature 68.0 °F |
65% RH; ASTM D257 |