Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.731 GPa | 106 ksi | ASTM D790 |
Quadrant EPP TIVAR® 88-2 ESD Black, Premium Lubricant Filled, Lower COF, Electro Static Dissipative Lining Material (ASTM Product Data Sheet) |
|||
Flexural Modulus | 0.731 GPa | 106 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N2000HL Nylon 6 (Cond) Information provided by Ravago. |
|||
Flexural Modulus | 0.731 GPa | 106 ksi | 1% secant; ASTM D790 |
ExxonMobil LL 8450 Rotational Molding Resin
(discontinued **) LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. This resin is ideally suited for applications that require optimum balance.. |
|||
Flexural Modulus | 0.730 GPa | 106 ksi | 1.3 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 155-1326 LMDPE Rotational Molding Resin Description: ICORENE 155-1326 is a linear medium density polyethylene developed for use in rotational molding. It has a great combination of stiffness and toughness in a resin that is easy processi.. |
|||
Flexural Modulus | 0.730 GPa | 106 ksi | 1.3 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 195-1326 LMDPE Rotational Molding Resin Description: ICORENE 195-1326 is a linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness. Ke.. |
|||
Flexural Modulus | 0.730 GPa | 106 ksi | ISO 178 |
Total Lumicene® mPE M 4041 UV Metallocene Polyethylene, Rotomolding Lumicene® mPE M 4041 UV is a new generation metallocene medium density polyethylene with hexene as comonomer.Lumicene® mPE M 4041 UV is intended for the manufacture of rotomolded items.Lumicene® .. |
|||
Flexural Modulus | 0.730 GPa | 106 ksi | ASTM D790 |
Covestro Baydur® 660 IBS Polyurethane Structural Foam RIM, Density 30 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Flexural Modulus | 0.731 GPa | 106 ksi | 1% secant; ASTM D790 |
ExxonMobil LLP8450.31 Rotational Molding Resin LProduct Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that requir.. |
|||
Flexural Modulus | 0.731 GPa | 106 ksi | ASTM D-790 |
CMT Materials REN Shape® 440 Tooling Board, Modeling Board, Adhesive Products CMT Materials offers the complete line of REN Shape tooling board, modeling board, and related adhesive products. Vacuum formers and thermoformers use these products as prototype and low volume prod.. |
|||
Flexural Modulus | 0.730 GPa | 106 ksi | ASTM D790 |
Arkema Group Pebax® 7233 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Flexural Modulus | 0.730 GPa | 106 ksi | ISO 178 |
Polimeri Europa Clearflex® RL 50 U Linear Medium Density Polyethylene Clearflex RL 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RL 50 U show good mecha.. |
|||
Flexural Modulus | 0.730 GPa | 106 ksi | ASTM D790 |
Reliance Industries Relene C31101 Polyethylene Steel pipe coating High Density Polyethylene grade. Contains a minimum 2% of well dispersed carbon black.Characteristics:excellent weathering resistance, excellent processability, excellent adhesio.. |