Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 5.00e+13 ohm | 5.00e+13 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® AD143 PC LEXAN AD143 is a medium viscosity, injection molding grade exhibiting low dust attraction. It is designed for applications with high optical requirements in terms of clarity and light transmission .. |
|||
Surface Resistance | 5.00e+13 ohm | 5.00e+13 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® AD143 PC (Asia Pacific) LEXAN AD143 is a medium viscosity, injection molding grade exhibiting low dust attraction. It is designed for applications with high optical requirements in terms of clarity and light transmission .. |
|||
Surface Resistance | 5.00e+13 ohm | 5.00e+13 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® AD143 PC (Europe-Africa-Middle East) LEXAN AD143 is a medium viscosity, injection molding grade exhibiting low dust attraction. It is designed for applications with high optical requirements in terms of clarity and light transmission .. |
|||
Surface Resistance | 5.00e+13 ohm | 5.00e+13 ohm | ASTM D 257 |
SABIC Innovative Plastics Lexan® AD4820 PC LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin.This data was supplied by SABIC-IP for the America.. |
|||
Surface Resistance | 5.00e+13 ohm | 5.00e+13 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® AD4820 PC (Europe-Africa-Middle East) LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin. |
|||
Surface Resistance | 5.00e+13 ohm | 5.00e+13 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® LUX2489D PC (Europe-Africa-Middle East) Lexan LUX2489D is a polycarbonate resin with high reflective properties, UV additive, medium viscosity, injection molding grade exhibiting low dust attraction. |
|||
Surface Resistance | 5.00e+13 ohm | 5.00e+13 ohm | ASTM D257 |
Solvay Specialty Polymers Amodel® AF-4133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced
(discontinued AMODEL AF-4133 V0 is a 33% glass reinforced grade of polyphthalamide (PPA) resin that was designed specifically to process with water-cooled molds and meet the requirements of most electrical/electr.. |
|||
Surface Resistance | 5.00e+13 ohm | 5.00e+13 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® AD4820 PC (Asia Pacific) LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin. |
|||
Surface Resistance | 5.00e+13 ohm | 5.00e+13 ohm | IEC 60093 |
DSM Akulon® K230-HXG6 Nylon 6-30% Glass Reinforced (European Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Surface Resistance | 5.00e+13 ohm @Temperature 90.0 °C |
5.00e+13 ohm @Temperature 194 °F |
95% RH, 48 hrs |
Chevron Phillips Ryton® R10-110BL Polyphenylene Sulfide Compound
(discontinued **) Black Polyphenylene Sulfide CompoundRyton® R10-110BL is a glass and mineral filled polyphenylene sulfide compound which provides a good combination of mechanical and electrical properties.Applicati.. |
|||
Surface Resistance | 5.00e+13 ohm | 5.00e+13 ohm | IEC 60093 |
Solvay TECHNYL® A 218 S40 Black 21 N PA66, 40% glass spheres, DRY Description: Polyamide 66, reinforced with 40% of glass spheres, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL ® A 218 S40 is used in all sectors of ind.. |
|||
Surface Resistance | 5.00e+13 ohm | 5.00e+13 ohm | IEC 60093 |
Solvay TECHNYL® B 230 PA66/6, DRY Description: Unreinforced and modified copolyamide 66/6, with high flexibility and improved impact resistance, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHN.. |
|||
Surface Resistance | 5.00e+13 ohm | 5.00e+13 ohm | IEC 60093 |
Solvay TECHNYL® B 238 Black 21 N PA66/6, DRY Description: Unreinforced and modified copolyamide 66/6, heat stabilized, with improved impact resistance, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 238 is particular.. |
|||
Surface Resistance | 5.00e+13 ohm | 5.00e+13 ohm | IEC 60093 |
Solvay TECHNYL® A 218 MT15 V 25 Black 21N PA66, 25/15% glass/mineral fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 218 MT15.. |
|||
Surface Resistance | 5.00e+13 ohm | 5.00e+13 ohm | IEC 60093 |
Solvay TECHNYL® A 216 S30 PA66, 30% glass spheres, DRY Description: Polyamide 66, reinforced with 30% of glass spheres, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 216 S30 is used in all sectors of industry, offering an.. |
|||
Surface Resistance | 5.00e+13 ohm | 5.00e+13 ohm | IEC 60093 |
Solvay TECHNYL® A 216 S40 PA66, 40% glass spheres, DRY Description: Polyamide 66, reinforced with 40% of glass spheres, for injection molding.Available in: EuropeProduct Applications: TECHNYL ® A 216 S40 is used in all sectors of industry, offering a.. |
|||
Surface Resistance | 5.00e+13 ohm | 5.00e+13 ohm | ASTM D249 |
PlastxWorld CEVIAN® E81 ABS Inherently Static Dissipative Transparent ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Surface Resistance | 5.00e+13 ohm | 5.00e+13 ohm | IEC 60093 |
Polyplastics Duracon® WR-01 Acetal Co-polymer (POM), Chlorine water resistance DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Surface Resistance | 5.00e+13 ohm | 5.00e+13 ohm | IEC 60093 |
DSM Akulon® K224-HG4 Nylon 6-20% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Surface Resistance | 5.00e+13 ohm @Temperature 20.0 °C |
5.00e+13 ohm @Temperature 68.0 °F |
65% RH; ASTM D257 |
Arkema Group Pebax® 7233 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Surface Resistance | >= 5.00e+13 ohm | >= 5.00e+13 ohm | |
CEN® Electronic Material CN Polyimide Film, 7 Mil Thickness CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca.. |
|||
Surface Resistance | >= 5.00e+13 ohm | >= 5.00e+13 ohm | ASTM D257 |
CEN® Electronic Material CV Polyimide Film, 6 Mil Thickness CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup.. |
|||
Surface Resistance | 5.00e+13 - 1.90e+15 ohm | 5.00e+13 - 1.90e+15 ohm | Average value: 5.12e+14 ohm Grade Count:4 |
Overview of materials for Acrylic, Cast This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Surface Resistance | >= 5.00e+13 ohm | >= 5.00e+13 ohm | |
CEN® Electronic Material CN Polyimide Film, 6 Mil Thickness CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca.. |
|||
Surface Resistance | >= 5.00e+13 ohm | >= 5.00e+13 ohm | ASTM D257 |
CEN® Electronic Material CV Polyimide Film, 7 Mil Thickness CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup.. |
|||
Surface Resistance | >= 5.00e+13 ohm | >= 5.00e+13 ohm | IEC 60093 |
BASF Ultradur B 6550 L PBT Ultradur B 6550 L is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes. |