Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Fusion | 63.0 J/g | 27.1 BTU/lb | ASTM E793 |
Eastman Vitiva PC715 PET
(discontinued **) Vitiva PET PC715 is an exceptionally clear PET polyester that contains a UV light protection package chemically bound to the backbone of the polymer. This non-extractable UV inhibitor absorbs damagi.. |
|||
Heat of Fusion | 63.0 J/g | 27.1 BTU/lb | ASTM E793 |
Eastman 15041 PET
(discontinued **) Voridian polymer 15041 is a PET thermoplastic polyester.Applications/UsesCrystallized PET (CPET) trays |
|||
Heat of Fusion | 63.0 J/g | 27.1 BTU/lb | ASTM E793 |
Eastman 7352 PET
(discontinued **) VORIDIAN PET thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. VORIDIAN PET polyester 73.. |
|||
Heat of Fusion | 63.0 J/g | 27.1 BTU/lb | ASTM E793 |
Eastman 9663 PET
(discontinued **) VORIDIAN PET 9663 is a PET homopolymer widely used in the heatset industry and is FDA approved for food contact in hotfill applications. Voridian PET 9663 has a wide processing window and it’s vers.. |
|||
Heat of Fusion | 63.0 J/g | 27.1 BTU/lb | ASTM D3417 |
Arkema Group Pebax® 7233 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Heat of Fusion | 63.0 J/g | 27.1 BTU/lb | 80°C to end of melting |
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer
(discontinued **) Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c.. |
|||
Heat of Fusion | 63.0 J/g | 27.1 BTU/lb | ASTM E793 |
Eastman 5214A PET
(discontinued **) Voridian PET 5214A is a bright and transparent amber homopolymer that meets light barrier requirements while maintaining the desirable attributes of PET. This resin is commonly used to mold containe.. |