Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group EVATANE® 20-20 Copolymer Ethylene - Vinyl Acetate

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer Arkema
Trade Name Evatane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group EVATANE® 20-20 Copolymer Ethylene - Vinyl Acetate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EVATANE® 20-20 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 20-20 is stabilized with antioxidants. The High Vinyl Acetate content of EVATANE® 20-20 brings softness, flexibility and polarity. EVATANE® 20-20 is compatible with tackifying resins and waxes. It’s a useful product for hot melt adhesives formulation. EVATANE® 20-20 can also be used as a matrix to produce foams, cable compounds or as a additive for bitumen.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.940 g/cc

@Temperature 23.0 °C
0.0340 lb/in³

@Temperature 73.4 °F
ISO 1183
Vinyl Acetate Content 19 - 21 %
19 - 21 %
FTIR (internal)
Melt Index of Compound 17 - 23 g/10 min

@Load 2.16 kg,
Temperature 190 °C
17 - 23 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
ASTM D2240
Tensile Strength at Break 14.0 MPa
2030 psi
ASTM D638
Elongation at Break 600 - 900 %
600 - 900 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 82.0 °C
180 °F
DSC
Vicat Softening Point 47.0 °C

@Load 0.999 kg
117 °F

@Load 2.20 lb
ISO 306
Ring & Ball Softening Point 127 °C
261 °F
ASTM E28
Processing Properties Metric English Comments
Processing Temperature <= 230 °C
<= 446 °F
Copyright © lookpolymers.com All Rights Reserved