Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Victrex® PEEK 450PF Fine Powder Grade

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Glass Fiber Filled
Manufacturer Victrex
Trade Name PEEK
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Victrex® PEEK 450PF Fine Powder Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, standard flow, FDA food contact compliant, color natural.Information provided by Victrex.
Physical Properties Metric English Comments
Bulk Density 0.300 g/cc
0.0108 lb/in³
ISO 1183
Density 1.30 g/cc
0.0470 lb/in³
ASISO 1183
Particle Size 50 µm
50 µm
Average; ISO 13320-1
Viscosity 350000 cP

@Temperature 400 °C
350000 cP

@Temperature 752 °F
ISO 11443
Mechanical Properties Metric English Comments
Tensile Strength, Yield 98.0 MPa
14200 psi
ISO 527
Elongation at Break 30 %
30 %
ISO 527
Tensile Modulus 4.00 GPa
580 ksi
ISO 527
Flexural Strength 160 MPa
23200 psi
ISO 178
Flexural Modulus 3.80 GPa
551 ksi
ISO 527
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
ISO 180/A
Izod Impact, Unnotched (ISO) NB
NB
ISO 180/U
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
ISO 11357
Glass Transition Temp, Tg 143 °C
289 °F
Onset; ISO 11357
150 °C
302 °F
Midpoint; ISO 11357
Processing Properties Metric English Comments
Processing Temperature 380 - 400 °C
716 - 752 °F
Dry Time 3.00 hour

@Temperature 150 °C
3.00 hour

@Temperature 302 °F
5.00 hour

@Temperature 120 °C
5.00 hour

@Temperature 248 °F
Users viewing this material also viewed the following: