Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 17 g/10 min @Load 5.00 kg, Temperature 230 °C |
17 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYabs T00 GF20 ABS, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 17 g/10 min @Load 2.16 kg, Temperature 260 °C |
17 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® MC5215 PC+ABS (Asia Pacific) |
|||
Melt Index of Compound | 17 g/10 min @Load 5.00 kg, Temperature 260 °C |
17 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Polykemi AB SCANBLEND FS7 F20 PBT/ASA Blend, Glass Fiber-Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Melt Index of Compound | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER (Asia Pacific) Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Melt Index of Compound | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® CFR9131 PC COPOLYMER Lexan* CFR9131 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and .. |
|||
Melt Index of Compound | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer (Europe-Africa-Middle East) 18 MFR LEXAN High Flow Ductile Copolymer |
|||
Melt Index of Compound | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer (Europe-Africa-Middle East) 18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
Melt Index of Compound | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® LUX9136C PC COPOLYMER (Asia Pacific) Lexan* LUX9136C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Melt Index of Compound | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® PC1800 PC (Asia Pacific) PC1800 resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel.. |
|||
Melt Index of Compound | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® PC1800R PC (Europe-Africa-Middle East) PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Melt Index of Compound | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® VR2020 PC (Europe-Africa-Middle East) VR2020 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Melt Index of Compound | 17 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
Kuraray HYBRAR® SC1 Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Melt Index of Compound | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics PC1800R PC (Asia Pacific) PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Melt Index of Compound | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics PC1803R PC (Asia Pacific) PC1803R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Melt Index of Compound | 17 g/10 min @Load 5.00 kg, Temperature 360 °C |
17 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM HU1000E PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (.. |
|||
Melt Index of Compound | 17 g/10 min @Load 5.00 kg, Temperature 265 °C |
17 g/10 min @Load 11.0 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific) Designed for outdoor telecommunications enclosure applications. |
|||
Melt Index of Compound | 17 g/10 min @Load 2.16 kg, Temperature 250 °C |
17 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® K4530 PBT (Europe-Africa-Middle East) 15% glass reinforced PBT, Hydrolytically stable, High flow, Automotive connectors. |
|||
Melt Index of Compound | 17 g/10 min @Load 5.00 kg, Temperature 265 °C |
17 g/10 min @Load 11.0 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Xenoy® 6620U PBT+PC PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance. |
|||
Melt Index of Compound | 17 g/10 min @Load 2.16 kg, Temperature 265 °C |
17 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Xenoy® X5410 PC+PET (Asia Pacific) Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta.. |
|||
Melt Index of Compound | 17 g/10 min @Load 2.16 kg, Temperature 265 °C |
17 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Xenoy® X5410 PC+PET (Europe-Africa-Middle East) Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta.. |
|||
Melt Index of Compound | 17 g/10 min @Load 5.00 kg, Temperature 300 °C |
17 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP THERMOCOMP ZFM3314 PPE (Europe-Africa-Middle East) glas, mineral filled PPE |
|||
Melt Index of Compound | 17 g/10 min @Load 5.00 kg, Temperature 360 °C |
17 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 1000E PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. US FDA and EU Food Contact compliant. |
|||
Melt Index of Compound | 17 g/10 min @Load 5.00 kg, Temperature 360 °C |
17 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 1000EF PEI Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant. |
|||
Melt Index of Compound | 17 g/10 min @Load 5.00 kg, Temperature 360 °C |
17 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 1000EF PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant. |
|||
Melt Index of Compound | 17 g/10 min | 17 g/10 min | 2.16/230; ASTM D1238 |
A. Schulman POLYAXIS® PD2000 Polypropylene DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E.. |
|||
Melt Index of Compound | 17 g/10 min @Temperature 230 °C |
17 g/10 min @Temperature 446 °F |
ASTM D1238 |
Toyobo PELPRENE™ S1002 Polyester TPE, Ultra Heat-resistant Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo. |
|||
Melt Index of Compound | 17 g/10 min | 17 g/10 min | 2.16/230; ASTM D1238 |
A. Schulman POLYAXIS® PD2000 Polypropylene DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E.. |
|||
Melt Index of Compound | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics PC1800R PC (Europe-Africa-Middle East) PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Melt Index of Compound | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics PC1803R PC (Europe-Africa-Middle East) PC1803R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |