Polymer Property : Melting Point = 82.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 82.0 - 94.0 °C
180 - 201 °F
ASTM D3418(DSC)
DuPont Nucrel® 535 Ethylene-Methacrylic Acid Copolymer Resin  (discontinued **)
Nucrel® 535 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for ..
Melting Point 82.0 °C
180 °F
by DSC; ASTM D3418
Westlake EMAC® SP2405 20% Ethylene-Methyl Acrylate Copolymer  (discontinued **)
Westlake EMAC® SP2405 is a 20% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperature are required. SP2405 provides..
Melting Point 82.0 °C
180 °F
Freezing Point via DSC/ASTM D3418
DuPont Elvax® 3129 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film  (discontinued **)
10 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra..
Melting Point 82.0 °C
180 °F
Freezing Point via DSC/ASTM D3418
DuPont Elvax® 3120 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
7.5 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dr..
Melting Point 82.0 °C
180 °F
Freezing Point via DSC/ASTM D3418
DuPont Nucrel® 910 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
8.7 wt% Methacrylic Acid.Nucrel® 0910 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment de..
Melting Point 82.0 °C
180 °F
TRN-14
Tipco Tipcolite® TPF 1911 - Cashew Nut (CNSL) Modified Phenolic Resin with 51 mm Norton Flow, with 7% Hexamine
Cashew Nut (CNSL) Modified Phenolic Resin with 51mm Norton FlowApplications: Nitrile RubberProcessing: CompoundingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Melting Point 82.0 °C
180 °F
by DSC; ASTM D3418
Westlake EMAC® SP2205 20% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® SP2205 is a 20% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP2205 provide..
Melting Point 82.0 °C
180 °F
by DSC; ASTM D3418
Westlake EMAC® SP2220 20% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® SP2220 is a 20% EMA copolymer designed for compounding, extrusion coating, tie-layers, and extrusions where flexibility, compatibility, low heat seal temperatures, or high coefficien..
Melting Point 82.0 °C
180 °F
ASTM D3418
Westlake EMAC® SP2255 17% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® SP2255 is a 17% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat s..
Melting Point 82.0 °C
180 °F
ASTM D3418
Westlake EMAC® SP2258 17% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® SP2258 is a 17% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat s..
Melting Point 82.0 °C
180 °F
DSC; ASTM-D3418
Westlake EMAC® SP2409 20% EMA Copolymer
Westlake EMAC� SP2409 is a 20% EMA copolymer designed for extrusion coating, tie-layers, and extrusions where flexibility, compatibility, low heat seal temperatures, or a high coefficient of fr..
Melting Point 82.0 °C
180 °F
DTA
DuPont™ Surlyn® 8020 Ionomer Resin, Sodium
Surlyn® 8020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
Melting Point 82.0 °C
180 °F
DSC
DuPont™ Surlyn® 9150 Ionomer Resin, Zinc
Surlyn® 9150 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The high MAA content and mi..
Melting Point 82.0 °C
180 °F
DSC
Arkema Group EVATANE® 20-20 Copolymer Ethylene - Vinyl Acetate
EVATANE® 20-20 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 20-20 is stabilized with antioxidants. The High Vinyl Acetate co..
Melting Point 82.0 °C
180 °F
by DSC
Westlake EMAC® SP 1257 Ethylene-Methyl Acrylate Copolymer  (discontinued **)
20% Methyl Acrylate Content. Characteristics: FDA Clearance for Packaging of Most Foods, Including Aseptic Packaging; Less Crystalline and Softer than Polyethylene; Excellent Heat Stability Allows ..
Melting Point 82.0 °C
180 °F
Melting point via DSC/ASTM D3418
DuPont Bynel® 2169 Anhydride-Modified Ethylene Acrylate Adhesive Resin  (discontinued **)
Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in..