Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 47.0 °C | 117 °F | 1kg load; ASTM D1525 |
Westlake EMAC® SP1400 Specialty Copolymer
(discontinued **) EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. Fo.. |
|||
Vicat Softening Point | 47.0 °C | 117 °F | 1000g; ASTM D-1525 |
ExxonMobil Escorene® LD-769 High EVA Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymer designed for high filler acceptance. Compounds produced from this resin have excellent flexibility and toughness.Appl.. |
|||
Vicat Softening Point | 47.0 °C | 117 °F | ASTM D1525 |
DuPont Elvax® 260 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Vicat Softening Point | 47.0 °C | 117 °F | ASTM D1525 |
Westlake EMAC® SP2220 20% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2220 is a 20% EMA copolymer designed for compounding, extrusion coating, tie-layers, and extrusions where flexibility, compatibility, low heat seal temperatures, or high coefficien.. |
|||
Vicat Softening Point | 47.0 °C | 117 °F | B (50N); ISO 306 |
Borealis Daplen™ EE015U TPO Compound Daplen EE015U is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE015U is a material with excellent impact /stiffness ratio. Thanks to its low th.. |
|||
Vicat Softening Point | 47.0 °C | 117 °F | ASTM D1525 and ISO 306/A |
ExxonMobil Exact™ 9061 Ethylene-based Plastomer Resin Product Description: Exact 9061 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P.. |
|||
Vicat Softening Point | 47.0 °C | 117 °F | ASTM D1525, ISO 306 |
DuPont™ Appeel® 20D867 Ethylene Acrylate DuPont™ Appeel 20D867 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe.. |
|||
Vicat Softening Point | 47.0 °C | 117 °F | Rate B, ASTM D1525-70 |
DuPont™ Surlyn® 8320 Ionomer Resin, Sodium Surlyn® 8320 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. This very low modulus sod.. |
|||
Vicat Softening Point | 47.2 °C | 117 °F | ASTM D1525 |
ExxonMobil OPTEMA™ TC 120 ExCo Ethylene Methyl Acrylate Product Description: Optema TC 120 is an ethylene methyl acrylate copolymer intended for extrusion coating, coextrusion coating and extrusion lamination where good interlayer adhesion between polyet.. |
|||
Vicat Softening Point | 47.1 °C | 117 °F | ASTM D1525 |
ExxonMobil Vistamaxx™ 6202 Propylene-based Elastomer Product Description: Vistamaxx 6202 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Catalyst Technology. It has excellent elastomeric properties, i.. |
|||
Vicat Softening Point | 47.1 °C | 117 °F | ASTM D1525 |
ExxonMobil Vistamaxx™ 6202FL Propylene-based Elastomer - Performance Film Product Description: Vistamaxx 6202FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution, and is produced us.. |
|||
Vicat Softening Point | 47.2 °C | 117 °F | ASTM D1525 |
ExxonMobil Escorene® UL 7520 Adhesive Application Resin Escorene Ultra UL 7520 is a high flow, 18.5% vinyl acetate copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesives, sealan.. |
|||
Vicat Softening Point | 47.0 °C @Load 0.999 kg |
117 °F @Load 2.20 lb |
ISO 306 |
Arkema Group EVATANE® 20-20 Copolymer Ethylene - Vinyl Acetate EVATANE® 20-20 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 20-20 is stabilized with antioxidants. The High Vinyl Acetate co.. |
|||
Vicat Softening Point | 47.0 °C @Load 0.999 kg |
117 °F @Load 2.20 lb |
ASTM D1525 |
Arkema Group LOTADER® 3410 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 3410 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. LOTADER 3410 is a versatile adhesive for extrusion coating or lam.. |
|||
Vicat Softening Point | 47.1 - 167 °C | 117 - 333 °F | Average value: 72.2 °C Grade Count:8 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Film Grade". Each property range of values reported is minimum a.. |
|||
Vicat Softening Point | 47.0 °C | 117 °F | ASTM D1525 |
Lubrizol Estane® 58252 Thermoplastic Polyurethane Type: Estane® 58252 is a 70A polyether-type thermoplastic polyurethane (TPU).Features: Formulated to have one of the highest MVT values within the thermoplastic polyurethane class. It is also amon.. |
|||
Vicat Softening Point | 47.0 °C | 117 °F | ASTM D1525 |
DuPont Elvax® 3175LG Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion
(discontinued **) 28 wt% Vinyl Acetate.Elvax® 3175 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Vicat Softening Point | 47.0 °C | 117 °F | ASTM D1525 |
DuPont Elvax® 3175 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion 28 wt% Vinyl Acetate.Elvax® 3175 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |