Minelco Reclaimed Mid Alumina

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Minelco Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Minelco Reclaimed Mid Alumina.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hand sorted material from the brickworks and steelworksApplications: Manufacture of low temperature castables
Component Elements Properties Metric English Comments
Al2O3 >= 55 %
>= 55 %