Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 16 - 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 - 23 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Chase Plastics CP Pryme® PC300HFR Polycarbonate (Utility Grade), High Flow, Mold Release Information provided by Chase Plastics. |
|||
Melt Index of Compound | 17 - 23 g/10 min @Load 2.16 kg, Temperature 190 °C |
17 - 23 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group EVATANE® 20-20 Copolymer Ethylene - Vinyl Acetate EVATANE® 20-20 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 20-20 is stabilized with antioxidants. The High Vinyl Acetate co.. |