Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aremco Aremco-Bond™ 598 Conductive Epoxy Adhesive  (discontinued **)

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive , Epoxy, Electrically Conductive
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Aremco-Bond™ 598 Conductive Epoxy Adhesive  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Electrically and thermally conductive, nickel-filled, single part system. Low viscosity, inorganic coating for applications to 1000 ºF (540 °C).
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
Mechanical Properties Metric English Comments
Adhesive Bond Strength 9.48 MPa
1370 psi
Per ASTM D1002-94; shear strength of single lap-joint metal coupons in tension loading.
Thermal Properties Metric English Comments
CTE, linear 33.7 µm/m-°C

@Temperature 20.0 °C
18.7 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 1.20 W/m-K
8.33 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 538 °C
1000 °F
Electrical Properties Metric English Comments
Electrical Resistivity 1e+05
1e+05
Dielectric Strength 9.80 kV/mm
249 kV/in
Processing Properties Metric English Comments
Pot Life 240 min
240 min
Users viewing this material also viewed the following: