Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.20 - 1.50 W/m-K | 8.33 - 10.4 BTU-in/hr-ft²-°F | |
Parker Chomerics CHO-BOND 584-208 Conductive Adhesive Two-component, highly conductive adhesive system that combines the good adhesive characteristics of epoxy with the superior conductivity of silver. In addition to being available in bulk form, the m.. |
|||
Thermal Conductivity | 1.20 - 1.50 W/m-K | 8.33 - 10.4 BTU-in/hr-ft²-°F | |
Parker Chomerics CHO-BOND 584-29 Conductive Adhesive Two-component, highly conductive adhesive system that combines the good adhesive characteristics of epoxy with the superior conductivity of silver. In addition to being available in bulk form, the m.. |
|||
Thermal Conductivity | 1.20 W/m-K @Pressure 2.07 MPa |
8.33 BTU-in/hr-ft²-°F @Pressure 300 psi |
ASTM D5470 |
Parker Chomerics CHO-SEAL 1298 EMI Shielding Material Corrosion Resistant EMI Shielding Gasket. Through the use of new proprietary particle painting and elastomer compounding technology, CHO-SEAL® 1298 shielding elastomer offers a six-fold increase in.. |
|||
Thermal Conductivity | 1.20 W/m-K @Pressure 2.07 MPa |
8.33 BTU-in/hr-ft²-°F @Pressure 300 psi |
ASTM D5470 |
Parker Chomerics CHO-SEAL 1350 Conductive Elastomer Standard material for high volume injection and compression molding and small extrusions; high performance in non-corrosive environments; used in grounding applications with little or no vibration.R.. |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | ASTM E 1530 |
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Europe-Africa-Middle East) LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | JIS-R-2618; ASTM D2326 |
Fujipoly Industries Sarcon® GR-c Gap Filler Pad Sarcon GR-c is a highly conformable, thermally conductive (no electric conductive) and electromagnetic wave absorption material in areas where space between surfaces is uneven and surface textures v.. |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | 150°C for 1,000 hrs; JIS-R-2618 |
Fujipoly Industries Sarcon® GR-c Gap Filler Pad Sarcon GR-c is a highly conformable, thermally conductive (no electric conductive) and electromagnetic wave absorption material in areas where space between surfaces is uneven and surface textures v.. |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | 70°C for 1,000 hrs; JIS-R-2618 |
Fujipoly Industries Sarcon® GR-c Gap Filler Pad Sarcon GR-c is a highly conformable, thermally conductive (no electric conductive) and electromagnetic wave absorption material in areas where space between surfaces is uneven and surface textures v.. |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | JIS-R-2618; ASTM D2326 |
Fujipoly Industries Sarcon® GR-k Gap Filler Pad Sarcon GR-k is a general type of thermal conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and mak.. |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | HOT-DISK || 60x60x3 mm |
Lehmann & Voss LUVOCOM® 1/CF/30 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | Longitudinal |
LATI Laticonther 62 CPG/500 PA 6, Glass Fiber Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Thermal Conductivity | 1.20 W/m-K @Temperature 90.0 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott DURATAN® Borosilicate Glass Prestressed borosilicate glass 3.3, chemically and thermally highly resistant, Flameproof lighting The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below .. |
|||
Thermal Conductivity | 1.20 W/m-K @Temperature 90.0 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott DUROBAX® amber Neutral Glass Tubing Neutral glass tubing, chemically highly resistant, with light protection Containers, test tubes, pipettes, chemical and technical apparatus The heavy metal content for the elements lead, cadmium, .. |
|||
Thermal Conductivity | 1.20 W/m-K @Temperature 90.0 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott Glass 8245 Borosilicate Glass Borosilicate glass for sealing to Kovar metal and molybdenum, minimum X-ray absorption, low self radiation, good insulator X-ray tubes, video-frequency tubes, photomultiplier tubes The heavy metal.. |
|||
Thermal Conductivity | 1.20 W/m-K @Temperature 90.0 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott Glass 8326 Neutral Glass Tubing Neutral glass tubing, alkali resistance better as for DURAN® Special lab glass The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is less than 100 ppm.Info.. |
|||
Thermal Conductivity | 1.20 W/m-K @Temperature 90.0 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott Glass 8688 Borosilicate Glass Borosilicate glass, highly UV-blocked, stabilized against solarization, sealing glass to Tungsten Backlights The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium.. |
|||
Thermal Conductivity | 1.20 W/m-K @Temperature 90.0 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott Glass 8689 Borosilicate Glass Borosilicate glass, highly UV-blocked, stabilized against solarization, sealing glass to Tungsten Backlights The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium.. |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | ISO 22007-4 |
Sichuan Deyang Haton® hFR70 PPS / AR Polyphenylene Sulfide Injection molding, themal conductionInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | |
Loctite® 3872 1 component acrylic/urethane UV/Heat Cure Flexible Adhesive Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or.. |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | |
Epoxy Technology EPO-TEK® B912-8 Epoxy Product Description: A single component, thermally and electrically conductive, epoxy adhesive designed for semiconductor die attach and circuit assembly applications. Its unique features are a pot.. |
|||
Thermal Conductivity | 1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | |
Epoxy Technology EPO-TEK® EM127 Electrically Conductive Epoxy Product Description: EPO-TEK® EM127 is a single component, heat curable, electrically conductive epoxy adhesive for semiconductor IC and LED die attach applications.Advantages & Application Notes: .. |
|||
Thermal Conductivity | >= 1.20 W/m-K | >= 8.33 BTU-in/hr-ft²-°F | |
Arlon 0.008" (0.2032 mm) Thermabond®-45 Uncured Silicone (99720W008) 0.008 in., +0.000,-0.002(0.2 mm, +0.00, -0.05) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.008 in +0.000,-0.002(0... |
|||
Thermal Conductivity | 1.20 - 3.20 W/m-K | 8.33 - 22.2 BTU-in/hr-ft²-°F | |
CeramTec Ceramtape GC Glass Ceramic LTCC (Low Temperature Cofired Ceramic) is a new type of ceramic film developed by CeramTec AG's Electronics division. With the aid of these ceramics and their almost shrinkage-free sintering process.. |
|||
Thermal Conductivity | 1.20 W/m-K @Temperature 90.0 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott CONTURAX® Borosilicate Glass Borosilicate glass tubing and rod, varying types of inner and outer shapes Lighting, giftware, and decoration The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromi.. |
|||
Thermal Conductivity | 1.20 W/m-K @Temperature 90.0 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott DUROBAX® clear Neutral Glass Tubing Neutral glass tubing, chemically highly resistant Syringes, cartridges, chemical and technical apparatus The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is.. |