Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 538 °C | 1000 °F | |
PSM Industries Ferro-TiC® CM-25 High Chrome Tool Steel Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Ferr.. |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | Continuous |
Pyrotek TS-450 Thermoset Electrical Insulation Product Glass reinforcement, Mica resin, Silver color. Highest temperature resistance. High dielectric properties.Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | |
PSM Industries Ferro-TiC® SK Impact Resistant Tool Steel Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Exce.. |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | |
Garlock 9900 Compressed Graphite Fiber Gasketing, Nitrile Binder Graphite fibers with a nitrile binder.Graphite fiber gasketing withstands extreme temperatures and pressures, as well as many chemicalsPassed Garlock Fire tests, and is ABS Fire Safe Type ApprovedLo.. |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | Fabric Limit, Continuous |
Mid-Mountain Materials ARMATEX® SF10 Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | Fabric Limit, Continuous |
Mid-Mountain Materials ARMATEX® SF17 Industrial Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | Fabric Limit, Continuous |
Mid-Mountain Materials ARMATEX® SF22 Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | Fabric Limit, Continuous |
Mid-Mountain Materials ARMATEX® SF32 Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | Fabric Limit, Continuous |
Mid-Mountain Materials ARMATEX® SF45 Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | Fabric Limit, Continuous |
Mid-Mountain Materials ARMATEX® SF90 Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | Continuous |
Mid-Mountain Materials CERMEX® MT1000 Needled Fiberglass Mat CERMEX® MT1000 fiberglass mat is comprised of high purity, highly resilient E-Glass fibers. CERMEX® MT1000 is lightweight, strong, and highly efficient as insulation in most high heat environm.. |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | Continuous |
Mid-Mountain Materials PADMAT® MT1000 Needled Fiberglass Mat Description: PADMAT® MT1000 fiberglass mat is comprised of high purity, high strength E-Glass fibers. These long fibers are mechanically needled into high strength, binderless insulation material.. |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | Fabric Limit, Continuous |
Mid-Mountain Materials ARMATEX® FF18 Fluoroelastomer Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | |
Chesterton 787 Sliding Paste Description: Chesterton® 787 Sliding Paste is a premium quality pure synthetic lubricant that will function affectivity even at ultra high temperatures and pressures. Designed for the most severe o.. |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | |
Aremco AREMCOLOX™ 502-1100 (Unfired) Machinable Alumino-Silicate Good thermal and dielectric properties and can be fired to increase temperature resistance and mechanical strength. Easily machined to close tolerances. Plates, rods and bars available to 12". |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | Continuous |
Aremco Glass-Coat™ GC4000 High Temperature Specialty Coatings Glass Glass-enamel, gloss-black coating for stainless steel to 1000°F (538°C) |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | Long Term |
TIMET TIMETAL® 6-2-4-2 (Ti-6Al-2Sn-4Zr-2Mo-0.08Si) Titanium Alloy Medium-Strength, Elevated Temperature AlloyIndustry Specifications: USA Aerospace: AMS 4919.Features: TIMETAL 6-2-4-2 has good tensile creep and fatigue properties up to 540°C. It is the most comm.. |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | |
Aremco Aremco-Bond™ 598 Conductive Epoxy Adhesive
(discontinued **) Electrically and thermally conductive, nickel-filled, single part system. Low viscosity, inorganic coating for applications to 1000 ºF (540 °C). |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | |
PSM Industries Ferro-TiC® CHW-25 Hot Work Tool Steel Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Ferr.. |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | |
PSM Industries Ferro-TiC® CHW-45 Hot Work Tool Steel Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Ferr.. |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | Ductility maintained well above this temp. |
ATI Allegheny Ludlum AL 825™ Nickel Alloy Allegheny Ludlum AL 825 alloy is an austenitic nickel-iron-chromium-molybdenum-copper alloy containing high levels of corrosion resistance to both moderately oxidizing and moderately reducing enviro.. |