Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 9.80 kV/mm | 249 kV/in | |
Pyrotek ISOMAG® 175 Structural Insulation Board Isomag® 70 is a high strength insulating board suitable as an electrical insulator or a thermal barrier material in a variety of industrial applications. Its magnesia silicate based formulation pr.. |
|||
Dielectric Strength | 9.80 kV/mm @Thickness 2.50 mm |
249 kV/in @Thickness 0.0984 in |
DC @ 0.100 in (2.5 mm) thickness |
MarkeTech Aluminum Oxide Ceramic - Alumina 99.5% Data provided by the supplier, MarkeTech International.Because of their high temperature, chemical, electrical, and mechanical properties along with their relatively low cost and ease of manufacture.. |
|||
Dielectric Strength | 9.80 kV/mm | 249 kV/in | Step by step; ASTM D149 |
Sumitomo Bakelite Durez® 31735 Phenolic, Compression Grade Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimension.. |
|||
Dielectric Strength | 9.80 kV/mm @Frequency 60.0 Hz |
249 kV/in @Frequency 60.0 Hz |
step-by-step, wet; ASTM D149 |
Sumitomo Bakelite North America EM 7302XLD Long Glass Fiber Reinforced Epoxy EM 7302XLD is a long fiberglass reinforced epoxy molding compound with a low density inert filler. This compound is designed for applications where moderate strength and weight savings are desirable.. |
|||
Dielectric Strength | 9.80 kV/mm | 249 kV/in | Step by step; ASTM D149 |
Sumitomo Bakelite Durez® 25378 Phenolic, Injection Grade Durez 25378 Black Phenolic is a two stage heat resistant/electrical grade molding material having an excellent molded finish, low shrinkage and good heat resistance. Durez 25378 has exceptional UL .. |
|||
Dielectric Strength | 9.80 kV/mm | 249 kV/in | Step by step; ASTM D149 |
Sumitomo Bakelite Durez® 31906 Phenolic, Injection Grade Durez 31906 Black Phenolic is an asbestos free, medium impact, molding compound. It is designed for applications where additional mechanical strength is required.Information provided by Sumitomo Ba.. |
|||
Dielectric Strength | 9.80 kV/mm | 249 kV/in | 60Hz, Short Time, wet; ASTM D149 |
Sumitomo Bakelite North America SI 9002N-1 Silicone Compound Short fibergass reinforced silicone molding compound which offers moderate strength properties, dimensional stability, and excellent long-term thermal stability at elevated temperatures.Information .. |
|||
Dielectric Strength | 9.80 kV/mm | 249 kV/in | Step by Step; ASTM D149 |
Plenco 00732 Melamine-Phenolic, Granular, Compression Molded PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 007.. |
|||
Dielectric Strength | 9.80 kV/mm | 249 kV/in | ac; ASTM D116 |
CoorsTek Mullite, S2 Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Dielectric Strength | 9.80 kV/mm | 249 kV/in | |
Du-Co Ceramics DC-265-L-6 Alumina, 96% Al2O3 Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Dielectric Strength | 9.80 kV/mm | 249 kV/in | ASTM D149 |
Chang Chun Plastic Longlite PM T33J General Purpose Phenolic Molding Compound ASTM Grades per ASTM D700 are 2,3.Information provided by Dowell Trading Company Ltd. |
|||
Dielectric Strength | 9.80 kV/mm | 249 kV/in | |
Aremco Aremco-Bond™ 598 Conductive Epoxy Adhesive
(discontinued **) Electrically and thermally conductive, nickel-filled, single part system. Low viscosity, inorganic coating for applications to 1000 ºF (540 °C). |
|||
Dielectric Strength | 9.80 kV/mm | 249 kV/in | Short Time; ASTM D149 |
Plenco 7321 Phenolic, Nodular, Injection Molded PLENCO 07321 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and excellent dimensional stability. Type ASTM 5948 CFI-5, and UL recognized under compon.. |
|||
Dielectric Strength | 9.80 kV/mm | 249 kV/in | ASTM D149 |
Chang Chun Plastic Longlite PM T385J General Purpose Phenolic Molding Compound ASTM Grades per ASTM D700 are 2, 3.Information provided by Dowell Trading Company Ltd. |
|||
Dielectric Strength | 9.80 kV/mm | 249 kV/in | 60Hz, Short Time, wet; ASTM D149 |
Sumitomo Bakelite North America SI 9002J-1 Silicone Compound SI 9002J-1 is a short fiberglass reinforced silicone molding compound, which offers moderate strength properties, and dimensional stability and excellent long-term thermal stability at elevated temp.. |