Material Notes:
STYRON® 613 high heat, high strength general purpose polystyrene is typically used in applications requiring a clear, tough part such as office products and magnetic media enclosures. It offers good moldability. When used unmodified for the manufacture of food contact articles STYRON 613 complies with the US Food, Drug and Cosmetic Act and Food Additive Regulations 21 CFR 177.1640. The regulations should be consulted for complete details.Data provided by Dow Chemical.Americas Styrenics was formed in 2008 as a joint venture between Dow Chemical and Chevron Phillips Chemical Company. Styron was a Dow trade name before the JV formation.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM Data
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
Melt Flow 1.4 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.4 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM Data
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 51.7 MPa
7500 psi
ASTM Data
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM Data
Elongation at Break 1.8 %
1.8 %
ASTM Data
Tensile Modulus 2.92 GPa
424 ksi
ASTM Data
Izod Impact, Notched 0.214 J/cm
0.401 ft-lb/in
ASTM Data
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
ASTM data
Deflection Temperature at 0.46 MPa (66 psi) 94.4 °C
202 °F
Unannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 81.7 °C
179 °F
Unannealed; ASTM Data
Vicat Softening Point 108 °C
226 °F
Flammability, UL94 HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Optical Properties Metric English Comments
Haze 1.0 %
1.0 %
Transmission, Visible 90 %
90 %