Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.92 GPa | 424 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® RCY6215 PC+ABS Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs. |
|||
Tensile Modulus | 2.92 GPa | 424 ksi | ASTM D638 |
Quadrant EPP Quadrant Nylon 612 |
|||
Tensile Modulus | 2.92 GPa | 424 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Cellular E2519 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Physical properties were measured on non-foamed profiles. Measured density of an extruded 1 thick free foamed part was 0.70 gms/cc at a 360 deg.F melt temperature.Information provided by PolyO.. |
|||
Tensile Modulus | 2.92 GPa | 424 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Dry Blend E7506 Polyvinyl Chloride, Rigid (PVC, Rigid) Geon E7506 is recommended for whites and light pastel colors only. Performs well in extrusion blow molding and high rate fencing capstock applications.Physical properties based on Geon E7506 white 1.. |
|||
Tensile Modulus | 2.92 GPa | 424 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Dry Blend E7755 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.92 GPa | 424 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Fittings 210(HR) Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.92 GPa | 423 ksi | 0.5 x 0.125 in. specimen; 0.2 in/min; ASTM D638 |
Americas Styrenics STYRON™ 666LR General Purpose Polystyrene Resin
(discontinued **) STYRON™ 666LR is a medium flow general purpose polystyrene specifically designed to blend with styrene butadiene styrene block copolymers for packaging applications requiring high clarity, improved.. |
|||
Tensile Modulus | 2.92 GPa | 424 ksi | ASTM Data |
Americas Styrenics Styron® 613 Polystyrene
(discontinued **) STYRON® 613 high heat, high strength general purpose polystyrene is typically used in applications requiring a clear, tough part such as office products and magnetic media enclosures. It offers goo.. |
|||
Tensile Modulus | 2.92 GPa | 424 ksi | ASTM Data |
Americas Styrenics Styron® 666D Polystyrene
(discontinued **) STYRON® 666D general purpose polystyrene resin is used in injection molding applications, particularly for medical, pharmaceutical and food uses. It offers excellent clarity, intermediate flow char.. |
|||
Tensile Modulus | 2.92 GPa | 424 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP IAL12 PA6.12 LNP* LUBRICOMP* IAL12 is a compound based on Nylon 6/12 resin containing 5% PTFE, 10% Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.92 GPa | 424 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP (Asia Pacific) LNP* Thermocomp* MH0500C is a compound based on Polypropylene resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Tensile Modulus | 2.92 GPa | 424 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP LNP* THERMOCOMP* MH0500C is a compound based on Polypropylene resin. Added feature of this material is: High Specific Gravity. |
|||
Tensile Modulus | 2.92 GPa | 424 ksi | Storage |
Epoxy Technology EPO-TEK® H35-175MPT Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H35MPT is a single component, silver-filled, electrically conductive epoxy designed for military hybrid die and component attach. High viscosity version of EPO-TEK® H.. |