Material Notes:
AboCast 8504-5 is a clear, plasticized one-component epoxy system with very high strength and impact. It provides exceptional physical properties and thermal shock resistance from sub-zero to moderately high temperatures. Suggested Uses: Casting; Potting; Encapsulating; Embedding applications where 2-component systems can not be used; Electronic and structural components, patterns, and medical equipment; Coating; Impregnation; Resurfacing; Insulation; Bonding metal, ceramics, glass, and most rigid materials; Assembly; Patching; and Filling.
Physical Properties Metric English Comments
Viscosity 1500 cP
1500 cP
Mechanical Properties Metric English Comments
Hardness, Rockwell M 95
95
Tensile Strength at Break 61.4 MPa
8900 psi
Elongation at Break 7.6 %
7.6 %
Flexural Strength 100 MPa
14500 psi
Flexural Modulus 3.03 GPa
440 ksi
Compressive Strength 279 MPa
40500 psi
Thermal Properties Metric English Comments
Thermal Conductivity 0.167 - 0.201 W/m-K
1.16 - 1.39 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 72.0 °C
162 °F
Deflection Temp at unknown load
Electrical Properties Metric English Comments
Volume Resistivity 1.51e+15 ohm-cm
1.51e+15 ohm-cm
C 96/23/96
3.77e+15 ohm-cm
3.77e+15 ohm-cm
"A"
Surface Resistance 1.02e+15 ohm
1.02e+15 ohm
C 96/23/96
1.57e+15 ohm
1.57e+15 ohm
Cond. A
Dielectric Constant 3.2

@Frequency 1.00e+6 Hz
3.2

@Frequency 1.00e+6 Hz
A
3.54

@Frequency 60.0 Hz
3.54

@Frequency 60.0 Hz
A
Processing Properties Metric English Comments
Cure Time 60.0 - 120 min

@Temperature 150 - 160 °C
1.00 - 2.00 hour

@Temperature 302 - 320 °F
60.0 - 240 min

@Temperature 160 - 180 °C
1.00 - 4.00 hour

@Temperature 320 - 356 °F
optional
Pot Life 220 min

@Temperature 100 °C
220 min

@Temperature 212 °F
Shelf Life 5.00 - 8.00 Month
5.00 - 8.00 Month
Users viewing this material also viewed the following: