Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Volume Resistivity = 3.77e+15 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 3.77e+15 ohm-cm
3.77e+15 ohm-cm
"A"
Abatron AboCast 8504-5 One-Component Epoxy
AboCast 8504-5 is a clear, plasticized one-component epoxy system with very high strength and impact. It provides exceptional physical properties and thermal shock resistance from sub-zero to modera..