Electrical Properties Metric English Comments
Volume Resistivity 1.51e+15 ohm-cm
1.51e+15 ohm-cm
C 96/23/96
Abatron AboCast 8504-5 One-Component Epoxy
AboCast 8504-5 is a clear, plasticized one-component epoxy system with very high strength and impact. It provides exceptional physical properties and thermal shock resistance from sub-zero to modera..