Processing Properties Metric English Comments
Pot Life 220 min

@Temperature 100 °C
220 min

@Temperature 212 °F
Abatron AboCast 8504-5 One-Component Epoxy
AboCast 8504-5 is a clear, plasticized one-component epoxy system with very high strength and impact. It provides exceptional physical properties and thermal shock resistance from sub-zero to modera..